A technology for water-based latex paint and air purification, applied in the field of latex paint, can solve the problems of poor storage stability, large amount of additives and solvents, and large indoor pollution, achieve stable performance, reduce the use of organic solvents, and improve indoor environmental quality Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
example 1
[0019] First, weigh 30g of talc powder, 20g of tourmaline and 10g of vermiculite and mix them to obtain a mixture. Mix the mixture with water according to the mass ratio of 1:2 and put it into a ball mill for 5 hours of ball milling. Dry at high temperature for 6 hours, continue grinding for 1 hour after drying, and pass through a 1000-mesh sieve to obtain a mixed powder; weigh 20 g of polyvinylpyrrolidone and add it to 100 mL of deionized water, and add 30 mL of absolute ethanol, stir and mix for 20 minutes, then add 15 g of the above mixed powder and 2g of triethanolamine, ultrasonically dispersed for 15min to obtain a suspension, set aside; weigh 40g of methyl methacrylate, 30g of n-butyl acrylate, 20g of acrylic acid, 5g of decamethylcyclopentasiloxane and 6g of vinyltriethoxy Mix silane to obtain mixed monomer, weigh 15g cocamide methyl, 8g lauryl ammonium sulfate and 3g sodium lauryl alcohol polyoxyethylene ether sulfate respectively to obtain mixed emulsifier, first weig...
example 2
[0022] First, weigh 40g of talc powder, 25g of tourmaline and 13g of vermiculite and mix them to obtain a mixture. Mix the mixture with water according to the mass ratio of 1:2 and put it into a ball mill for ball milling for 6 hours. Dry at high temperature for 7 hours, continue to grind for 1.5 hours after drying, and pass through a 1100 mesh sieve to obtain a mixed powder; weigh 30g of polyvinylpyrrolidone and add it to 125mL of deionized water, and add 40mL of absolute ethanol, stir and mix for 25min, then add 17g of the above mixed powder and 2.5g triethanolamine, ultrasonically dispersed for 17min to obtain a suspension, and set aside; respectively weigh 45g methyl methacrylate, 33g n-butyl acrylate, 25g acrylic acid, 8g decamethylcyclopentasiloxane and 7g vinyl triethyl Oxysilane is mixed to obtain a mixed monomer, and 17g of cocamide methyl, 9g of ammonium lauryl sulfate and 4g of sodium lauryl alcohol polyoxyethylene ether sulfate are weighed respectively to obtain a m...
example 3
[0025] First, weigh 50g of talcum powder, 30g of tourmaline and 15g of vermiculite and mix them to obtain a mixture. Mix the mixture with water according to the mass ratio of 1:2 and put it into a ball mill for 7 hours of ball milling. Dry at high temperature for 8 hours, continue to grind for 2 hours after drying, and pass through a 1200 mesh sieve to obtain a mixed powder; weigh 40g of polyvinylpyrrolidone and add it to 150mL of deionized water, and add 50mL of absolute ethanol, stir and mix for 30min, then add 20g of the above mixed powder and 3g of triethanolamine, ultrasonically dispersed for 20min to obtain a suspension, set aside; weigh 50g of methyl methacrylate, 35g of n-butyl acrylate, 30g of acrylic acid, 10g of decamethylcyclopentasiloxane and 8g of vinyltriethoxy Mix the silane to obtain a mixed monomer, weigh 20g of cocamide methyl, 10g of ammonium lauryl sulfate and 5g of sodium lauryl alcohol polyoxyethylene ether sulfate respectively to obtain a mixed emulsifie...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com