Embodiment 1
[0036] The preparation of embodiment 1 value-added urea
[0037] A preparation method of value-added urea capable of activating soil, comprising the following steps:
[0038] (1) Put 80kg of urea into the melting tank for melting, and control the temperature at 115°C;
[0039] (2) Put 15kg of humic acid, 16kg of alginic acid, 2.5kg of HEDP, and 3.6kg of PVA into the urea melting tank, and stir for 2 minutes;
[0040] (3) Add 6.8 kg of zinc oxide into the melting tank, stir for 15 minutes, and then spray it into the prilling tower through a special nozzle for granulation to obtain value-added urea 1.
Embodiment 2
[0042] A preparation method of value-added urea capable of activating soil, comprising the following steps:
[0043] (1) Put 60kg of urea into the melting tank for melting, and control the temperature at 115°C;
[0044] (2) Put 16kg of brown humic acid, 20kg of alginic acid, 5.5kg of PAM, and 3.5kg of DTPMP into the urea melting tank, and stir for 2 minutes;
[0045] (3) Add 2 kg of zinc oxide, 3 kg of calcium oxide, and 4 kg of magnesium oxide into the melting tank, stir for 15 minutes, and then spray into the prilling tower through a special nozzle for granulation to obtain value-added urea 2.
Embodiment 3
[0047] A preparation method of value-added urea capable of activating soil, comprising the following steps:
[0048] (1) Put 70kg of urea into the melting tank for melting, and control the temperature at 115°C;
[0049] (2) Put 8 kg of fulvic acid, 5 kg of chitosan, 2.5 kg of gluconic acid, 3.5 kg of PVA, and 1.5 kg of PAM into the urea melting tank, and stir for 3.5 min;
[0050] (3) Add 3 kg of zinc oxide and 4 kg of iron oxide into the melting tank, stir for 15 minutes, and then spray into the prilling tower through a special nozzle for granulation to obtain value-added urea 3 .