Embodiment 1
[0017] Embodiment 1: adopt following steps to make oil paint:
[0018] Step 1: Dissolving 0.5kg beeswax and 0.5kg vegetable cellulose in 30kg linseed oil;
[0019] Step 2: Add 40kg of colorant and 3.5kg of nano-titanium dioxide into the stirring tank and mix and stir for 30 minutes;
[0020] Step 3: Add 20kg nano-calcium carbonate, 5kg nano-zinc oxide and 3.5kg manganese dioxide to the mixing tank in step 2 and continue mixing and stirring for 30-60 minutes;
[0021] Step 4: Add the solution in Step 1 to the stirring tank of Step 2 and continue mixing and stirring for 30-60 minutes;
[0022] Step 5: Add the evenly stirred mixture in Step 4 into a grinder, and grind for 20-40 minutes to make oil paint.
Embodiment 2
[0023] Embodiment 2: adopt following steps to make oil paint:
[0024] Step 1: 2kg beeswax and 1.5kg vegetable cellulose are dissolved in 35kg linseed oil;
[0025] Step 2: Add 30kg of color material and 5kg of nano-titanium dioxide into the mixing tank and mix for 30-60 minutes;
[0026] Step 3: Add 18kg nano-calcium carbonate, 7kg nano-zinc oxide and 1.5kg manganese dioxide to the mixing tank in step 2 and continue mixing and stirring for 30-60 minutes;
[0027] Step 4: Add the solution in Step 1 to the mixing tank in Step 3 and continue mixing and stirring for 30-60 minutes;
[0028] Step 5: Add the evenly stirred mixture in Step 4 into a grinder, and grind for 10-40 minutes to make oil paint.
Embodiment 3
[0029] Embodiment 3: adopt following steps to make oil paint:
[0030] Step 1: 1kg beeswax and 1kg vegetable cellulose are dissolved in 40kg sunflower oil;
[0031] Step 2: Add 34kg of color material and 4kg of nano-titanium dioxide into the mixing tank and mix for 30-60 minutes;
[0032] Step 3: Add 15kg nano-calcium carbonate, 4kg nano-zinc oxide and 1kg manganese dioxide to the mixing tank in step 2 and continue mixing and stirring for 30-60 minutes;
[0033] Step 4: Add the solution in Step 1 to the mixing tank in Step 3 and continue mixing and stirring for 30-60 minutes;
[0034] Step 5: Add the evenly stirred mixture in Step 4 into a grinder, and grind for 10-40 minutes to make oil paint.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com