A handicraft and iron technology, which is applied to the device, coating, pretreatment surface, etc. for applying liquid to the surface, which can solve the problems of discarding rusty iron handicrafts, oxidation reaction of iron handicrafts, waste of resources and living costs, etc. , to achieve the effect of improving rust removal ability, improving gloss and reducing corrosion rate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] A method for derusting iron handicrafts, comprising the following steps:
[0023] (1) Degrease: Add sodium bicarbonate and sodium hydroxide to the water, heat to 55°C and cook for 6 minutes, immerse the rusty crafts in the solution and cook for 18 minutes, then add hydrochloric acid solution to neutralize the solution to pH7.0-7.5, then Add 7.2% of its mass degreasing agent to the water, heat to 73°C and boil for 27 minutes, and get the degreasing handicraft after cooling;
[0024] (2) High-temperature derusting: add water to carbon black powder and stir to make carbon black viscous liquid, use a paint brush to paint a layer of carbon black viscous liquid on the degreasing handicraft, and place it at 44°C for semi-drying Dry, then immerse in the yellow mud mixture for 2.5 minutes, take it out and place it in a high-temperature furnace for processing. The temperature of the high-temperature furnace is 217°C, the temperature rise rate is 13°C / min, and the heating time is ...
Embodiment 2
[0038] A method for derusting iron handicrafts, comprising the following steps:
[0039] (1) Degrease: Add sodium bicarbonate and sodium hydroxide to the water, heat to 57°C and cook for 7 minutes, immerse the rusty handicraft in the solution and cook for 19 minutes, then add hydrochloric acid solution to neutralize the solution to pH7.0-7.5, Then add a degreasing agent with a mass of 8.5% to the water, heat it to 75°C and boil for 29 minutes, and get a degreasing handicraft after cooling;
[0040] (2) High-temperature derusting: add water to carbon black powder and stir to make carbon black viscous liquid, use a paint brush to paint a layer of carbon black viscous liquid on the degreasing handicraft, and place it at 46°C for semi-drying dry, then immerse in the yellow mud mixture for 3 minutes, take it out and place it in a high-temperature furnace for processing. To 34°C, the cooling rate is 8°C / min; after cooling, brush the surface of the handicraft, and then paint the car...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com