[0036] Example 1
[0037] A cadmium-removing adsorbent for seafood, comprising the following raw materials by weight: 20 parts of modified silica powder, 50 parts of fish bone powder, 25 parts of modified shell powder, 15 parts of shrimp shell powder, 10 parts of sodium gluconate, and sodium carbonate 3 parts, 200 parts of solvent.
[0038] Wherein, the described modified silica powder is processed through the following steps:
[0039] a. Wash the silica powder with water, then dry it, soak it in 0.5M dilute hydrochloric acid for 24h, and then dry it;
[0040] b. Add magnesium chloride to water to configure 1M magnesium chloride solution, then add sodium hydroxide solution to the solution to make it a magnesium hydroxide suspension;
[0041] c. Put the silica powder obtained in step a into the magnesium hydroxide suspension obtained in step b and soak for 48h, stir once every 2h, take out the treated silica powder and bake at 110°C Dry;
[0042] d. The silica powder obtain...
Example Embodiment
[0052] Example 2
[0053] A cadmium-removing adsorbent for seafood, comprising the following raw materials in parts by weight: 30 parts of modified silica powder, 70 parts of fish bone powder, 50 parts of modified shell powder, 30 parts of shrimp shell powder, 30 parts of sodium gluconate, and sodium carbonate 5 parts and 200 parts of solvent.
[0054] Wherein, the described modified silica powder is processed through the following steps:
[0055] a. Wash the silica powder with water, then dry it, soak it in 0.5M dilute hydrochloric acid for 24h, and then dry it;
[0056] b. Add magnesium chloride to water to configure 1M magnesium chloride solution, then add sodium hydroxide solution to the solution to make it a magnesium hydroxide suspension;
[0057] c. Put the silica powder obtained in step a into the magnesium hydroxide suspension obtained in step b and soak for 48h, stir once every 2h, take out the treated silica powder and bake at 110°C Dry;
[0058] d. The silica p...
Example Embodiment
[0068] Example 3
[0069] A cadmium-removing adsorbent for seafood, comprising the following raw materials by weight: 25 parts of modified silica powder, 60 parts of fish bone powder, 36 parts of modified shell powder, 20 parts of shrimp shell powder, 20 parts of sodium gluconate, and sodium carbonate 4 parts, 200 parts of solvent.
[0070] Wherein, the described modified silica powder is processed through the following steps:
[0071] a. Wash the silica powder with water, then dry it, soak it in 0.5M dilute hydrochloric acid for 24h, and then dry it;
[0072] b. Add magnesium chloride to water to configure 1M magnesium chloride solution, then add sodium hydroxide solution to the solution to make it a magnesium hydroxide suspension;
[0073] c. Put the silica powder obtained in step a into the magnesium hydroxide suspension obtained in step b and soak for 48h, stir once every 2h, take out the treated silica powder and bake at 110°C Dry;
[0074] d. The silica powder obtain...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap