Environment-friendly floor tile for garden design and preparation method of environment-friendly floor tile
A floor tile and environmental protection technology, applied in the field of floor tiles, can solve the problems of underutilization, environmental pollution, waste of resources, etc., and achieve the effects of light weight, lower production costs, and less pollution
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] An environment-friendly floor tile for garden design, comprising the following raw materials in parts by weight:
[0028] 20 parts of waste bricks and tiles, 8 parts of waste glass, 8 parts of blast furnace slag, 15 parts of fly ash, 6 parts of diatomaceous earth, 6 parts of calcium carbonate, 4 parts of barium sulfate, 4 parts of bamboo charcoal powder, 15 parts of cement, and 4 parts of nano-titanium dioxide 4 parts of silk fibroin fiber, 5 parts of boron fiber, 3 parts of nano-zirconia, 3 parts of blackstone powder, 3 parts of magnesium hydroxide, 18 parts of water glass, 1.5 parts of water reducing agent, 1.5 parts of air-entraining agent, slow 0.8 parts of coagulant and 15 parts of water.
[0029] The water reducer is a polycarboxylate water reducer.
[0030] The air-entraining agent is rosinic acid.
[0031] The retarder is lignin.
[0032] This embodiment also discloses a preparation method of the above-mentioned environment-friendly floor tiles for garden des...
Embodiment 2
[0040] An environment-friendly floor tile for garden design, comprising the following raw materials in parts by weight:
[0041] 30 parts of waste bricks and tiles, 15 parts of waste glass, 15 parts of blast furnace slag, 25 parts of fly ash, 12 parts of diatomaceous earth, 12 parts of calcium carbonate, 9 parts of barium sulfate, 9 parts of bamboo charcoal powder, 22 parts of cement, and 9 parts of nano-titanium dioxide 9 parts of silk fibroin fiber, 10 parts of boron fiber, 8 parts of nano-zirconia, 8 parts of blackstone powder, 8 parts of magnesium hydroxide, 26 parts of water glass, 3 parts of water reducing agent, 3 parts of air-entraining agent, slow 1.8 parts of coagulant and 20 parts of water.
[0042] The water reducer is a polycarboxylate water reducer.
[0043] Air-entraining agents are aromatic hydrocarbons.
[0044] Retarders are phosphates.
[0045] This embodiment also discloses a preparation method of the above-mentioned environment-friendly floor tiles for ...
Embodiment 3
[0053] An environment-friendly floor tile for garden design, comprising the following raw materials in parts by weight:
[0054] 24 parts of waste bricks and tiles, 10 parts of waste glass, 10 parts of blast furnace slag, 18 parts of fly ash, 8 parts of diatomaceous earth, 8 parts of calcium carbonate, 5 parts of barium sulfate, 5 parts of bamboo charcoal powder, 18 parts of cement, and 5 parts of nano-titanium dioxide 5 parts of silk fibroin fiber, 6 parts of boron fiber, 4 parts of nano-zirconia, 4 parts of blackstone powder, 4 parts of magnesium hydroxide, 21 parts of water glass, 2 parts of water reducing agent, 2 parts of air-entraining agent, slow 1.3 parts of coagulant and 17 parts of water.
[0055] The water reducer is a polycarboxylate water reducer.
[0056] Air-entraining agents are aromatic alcohols.
[0057] Retarders are tartrates.
[0058] This embodiment also discloses a preparation method of the above-mentioned environment-friendly floor tiles for garden des...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com