Manufacturing method of environmentally-friendly three-ply board
A production method and technology of plywood, which is applied in the field of wood processing, can solve the problem of large formaldehyde release from plywood, achieve low peel strength, improve thermal stability, and improve overall performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] A method for making environmentally friendly plywood, comprising the following steps:
[0028] (1) Drying of the veneer: drying the veneer so that the moisture content of the veneer is 10%; the veneer includes a core board, a front board and a back board.
[0029] (2) Embryo grouping treatment: Coat the front and back of the core board treated in step (1) with a special adhesive, and stick the front board and the back board to the center board respectively. The front and back of the core board to obtain the blank. The weight of applying the special adhesive per square meter of the core board is 240g. The special adhesive is prepared from the following raw materials in parts by weight: 60 parts of phenolic glue, 30 parts of soybean protein glue, 30 parts of polyvinyl alcohol, 6 parts of starch, 2 parts of borax, 8 parts of sodium hydroxide and 30 parts of talcum powder . Wherein, the preparation method of described phenolic glue comprises the steps:
[0030] A1. Prep...
Embodiment 2
[0039] A method for making environmentally friendly plywood, comprising the following steps:
[0040] (1) Drying of the veneer: drying the veneer so that the moisture content of the veneer is 5%; the veneer includes a core board, a front board and a back board.
[0041] (2) Embryo grouping treatment: Coat the front and back of the core board treated in step (1) with a special adhesive, and stick the front board and the back board to the center board respectively. The front and back of the core board to obtain the blank. The weight of applying the special adhesive per square meter of the core board is 180g. The special adhesive is prepared from the following raw materials in parts by weight: 50 parts of phenolic glue, 20 parts of soybean protein glue, 20 parts of polyvinyl alcohol, 4 parts of starch, 1 part of borax, 5 parts of sodium hydroxide and 20 parts of talcum powder . Wherein, the preparation method of described phenolic glue comprises the steps:
[0042] A1. Prepar...
Embodiment 3
[0051] A method for making environmentally friendly plywood, comprising the following steps:
[0052] (1) Drying of the veneer: drying the veneer so that the moisture content of the veneer is 8%; the veneer includes a core board, a front board and a back board.
[0053] (2) Embryo grouping treatment: Coat the front and back of the core board treated in step (1) with a special adhesive, and stick the front board and the back board to the center board respectively. The front and back of the core board to obtain the blank. The weight of applying the special adhesive per square meter of the core board is 210g. The special adhesive is prepared from the following raw materials in parts by weight: 55 parts of phenolic glue, 25 parts of soybean protein glue, 25 parts of polyvinyl alcohol, 5 parts of starch, 1.5 parts of borax, 6.5 parts of sodium hydroxide and 25 parts of talcum powder . Wherein, the preparation method of described phenolic glue comprises the steps:
[0054] A1. P...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com