A sewage treatment agent and coating type technology, applied in the field of coating type sewage treatment agent and its preparation, can solve the problems of poor physical method treatment effect, high biological method treatment cost, secondary pollution of reagent components, etc., and achieve improvement. Surface activity, high recycling rate and good stability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A kind of coating type sewage treatment agent, it is made up of the raw material of following weight part:
[0022] Carboxymethylcellulose sodium 20, oxidized polyethylene wax 6, 2-mercaptobenzimidazole 1, saturated octadecylamide 2, mannitol 5, modified sol 40, calcium zeolite 90, polyacrylamide 14.
[0023] Described modified sol is made up of the raw material of following parts by weight:
[0024] Aluminum Isopropoxide 30, Vinyl Distearamide 2, Trimethylolpropane 3, Isopropanol 7.
[0025] The preparation method of described modified sol comprises the following steps:
[0026] (1) Take isopropanol, add it to deionized water 20 times its weight, stir evenly, raise the temperature to 55-60°C, add trimethylolpropane, keep stirring for 12 minutes, and obtain an alcohol dispersion;
[0027] (2) Take aluminum isopropoxide, add it to 30 times its weight in deionized water, stir evenly, mix with the above-mentioned alcohol dispersion, stir and react for 4 hours, add vinyl ...
Embodiment 2
[0034] A kind of coating type sewage treatment agent, it is made up of the raw material of following weight part:
[0035] Carboxymethylcellulose sodium 16, oxidized polyethylene wax 4, 2-mercaptobenzimidazole 0.7, saturated octadecylamide 1, mannitol 3, modified sol 30, calcium zeolite 70, polyacrylamide 10.
[0036] Described modified sol is made up of the raw material of following parts by weight:
[0037] Aluminum Isopropoxide 20, Vinyl Distearamide 1, Trimethylol Propane 2, Isopropanol 5.
[0038] The preparation method of described modified sol comprises the following steps:
[0039] (1) Take isopropanol, add it to deionized water 13 times its weight, stir evenly, raise the temperature to 55-60°C, add trimethylolpropane, keep stirring for 4 minutes, and obtain an alcohol dispersion;
[0040] (2) Take aluminum isopropoxide, add it to 25 times its weight in deionized water, stir evenly, mix with the above-mentioned alcohol dispersion, stir and react for 3 hours, add viny...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com