Air spring sealing ring for vehicle
A sealing ring, gas spring technology, applied in mechanical equipment, engine components, piston rings, etc., can solve the problems of poor durability, wear, long auxiliary time, etc., achieve excellent corrosion resistance, excellent mechanical properties, and improve mechanical properties. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0028] Please refer to Figure 1-2 As shown, the technical solution adopted in the present invention is: a gas spring sealing ring for automobiles, the main structure of the gas spring sealing ring 1 is set as a rubber jacket 2, and a soft metal mesh 3 is arranged in the rubber jacket 2, so that The inside of the soft metal mesh 3 is provided with metal reinforcing ribs 4, the rubber jacket 2 is provided with buffer holes 6 at both ends of the soft metal mesh 3, and the inner periphery of the rubber jacket 2 is provided with a hard support frame 5, so Sealing protrusions 7 are provided at the seals at both ends of the rubber jacket 2, and fastening grooves 8 are provided on the outer periphery of the rubber jacket 2;
[0029] The buffer holes 6 at the single end of the rubber jacket 2 are provided with 7 pieces, the shape is a hexagonal structure with a center, and the buffer holes 6 are independent of each other without communication
[0030] The rubber jacket 2 specifically...
Embodiment 2
[0037] The difference between this embodiment and embodiment 1 is:
[0038]The rubber jacket 2 specifically includes the following components in parts by weight: 30 parts of fluororubber raw rubber, 15 parts of rubber-plastic alloy, 30 parts of natural rubber, 6 parts of spidroin, 5 parts of 4-pentylphenylboronic acid, amidine phosphate 3 parts of base urea, 3 parts of stearic acid, 1 part of zinc stearate, 2 parts of black carbon black, 1 part of protective agent, 2 parts of modified glass fiber, 0.8 part of composite filler, 0.3 part of modified nano silver fiber, anti 0.6 parts of oxygen agent, 0.1 part of anti-aging agent, 0.1 part of accelerator and 1.3 parts of vulcanizing agent;
[0039] The modified glass fiber includes materials in the following percentages by weight: 90% of ordinary glass; 10% of ultraviolet absorber;
[0040] Among them, ordinary glass: SiO 2 60%;Na 2 O 10%; CaO 5%; MgO 2%; Al 2 o 3 2%;K 2 O 2%; B 2 o 3 19%;
[0041] UV absorber: γ-FeO(O...