Method for improving dyeing performance of real silk fiber based on enzymatic modification
A technology for dyeing performance and real silk, which is applied in dyeing methods, textiles and papermaking. It can solve the problems of limited types and quantities, low dyeing depth, and inability to meet the processing requirements of high-color-depth fabrics, and achieve high dyeing depth and fastness. degree, dyeing performance is obvious, the effect of mild reaction conditions
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] Select real silk electric spinning, carry out enzymatic real silk fiber modification and cationic dye dyeing with the method mentioned in the present invention;
[0027] (1) Enzymatic conversion of amino acids in silk: silk fibers are treated with serine hydroxymethyltransferase;
[0028] Treatment process prescription and conditions: Serine hydroxymethyltransferase 2.5U / mL, pyridoxal 5-phosphate 0.25mmol / L, tetrahydrofolate 2mmol / L, formaldehyde 5mmol / L, pH 7.5, temperature 30°C, treatment time 1 hours; after the treatment, the silk fibers are washed;
[0029] (2) protein kinase A catalyzed phosphorylation: the silk fiber treated in step (1) is catalyzed by protein kinase A for phosphorylation;
[0030] Treatment process prescription and conditions: protein kinase A 2.5U / mL, adenosine triphosphate 10mmol / L, cyclic adenosine monophosphate 1mmol / L, pH 6.5, temperature 25°C, treatment time 4 hours; after the treatment, the silk fibers were washed and dried.
[0031] (3)...
Embodiment 2
[0037] Select real silk knitted silk, carry out the cationic dyeing of real silk fiber with the method mentioned in the present invention;
[0038] (1) Enzymatic conversion of amino acids in silk: silk fibers are treated with serine hydroxymethyltransferase;
[0039] Treatment process prescription and conditions: Serine hydroxymethyltransferase 10U / mL, pyridoxal 5-phosphate 1mmol / L, tetrahydrofolate 8mmol / L, formaldehyde 12.5mmol / L, pH 8, temperature 37°C, treatment time 8 hours ;After the treatment, the silk fiber is washed with water;
[0040] (2) protein kinase A catalyzed phosphorylation: the silk fiber treated in step (1) is catalyzed by protein kinase A for phosphorylation;
[0041] Treatment process prescription and conditions: protein kinase A 10U / mL, adenosine triphosphate 50mmol / L, cyclic adenosine monophosphate 8mmol / L, pH 7.5, temperature 40°C, treatment time 10 hours; after the treatment, the silk fibers were washed and dried.
[0042] (3) Dyeing with cationic d...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com