A technology for landfill leachate and sludge conditioning, applied in sludge treatment, water/sludge/sewage treatment, dehydration/drying/concentrated sludge treatment, etc. Conditioning and modifying agents cannot be used to achieve the effect of increasing the water effluent speed and reducing the specific resistance of sludge
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] The solid content of the sludge produced by landfill leachate is 3.5%, the pH is neutral, and the mud is earthy red.
[0021] The conditioning modification tank is 50 cubic meters, and the paddle type stirring speed is 80 rpm.
[0022] The filling coefficient of the conditioning modified tank is 70%, that is, the amount of sludge per tank is 35 cubic meters.
[0023] According to the 4.0% (DS) ratio, the dosing amount of the new organic composite conditioning modifier is 49 kg, and diluted with water to 2000 kg, at this time the concentration of the modifier is 2.45%.
[0024] Add the diluted agent into the modified tank through the delivery pump, and stir until dense and stable flocs are formed.
[0025] According to the 20% (DS) ratio, the dosing amount of the solid skeleton powder is 245 kg, and it is added into the modified tank and stirred evenly.
[0026] The conditioned and modified sludge is transported to a 300-square-diaphragm plate filter press through a sc...
Embodiment 2
[0029] The landfill leachate sludge has a water content of 80% and a water content of 98.5% and is mixed according to a certain ratio. After mixing, the solid content of the sludge is 5.0%, the pH is neutral, and the mud is black.
[0030] The conditioning modification pool is 100 cubic meters, and the paddle-type stirring speed is 80 rpm.
[0031] The charging coefficient of the conditioning modified tank is 70%, that is, the amount of sludge in each tank is 70 cubic meters.
[0032] According to the proportion of 3.0% (DS), the dosing amount of the new organic compound conditioning modifier is 105 kg, and diluted with water to 4000 kg, at this time the concentration of the modifier is 2.62%.
[0033] Add the diluted agent into the modified tank through the delivery pump, and stir until dense and stable flocs are formed.
[0034] According to the ratio of 10% (DS), the dosing amount of solid skeleton powder is 350 kg, and it is added into the modified tank and stirred evenly...
PUM
Property | Measurement | Unit |
---|---|---|
particle size (mesh) | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com