A non-pickling chrome tanning agent
A technology of acid chrome tanning agent and sulfuric acid, which is applied in the field of leather chemical material preparation to achieve the effects of wide sources, good tanning effect and wide application range
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0035] After dissolving a certain amount of potassium dichromate in water, add sulfuric acid so that the ratio of the amount of chromium trioxide and sulfuric acid in the solution is 1:2.5; Mix the ethanol evenly, and add 50% of the mixed total alcohol into the acidic potassium dichromate solution evenly within 15 minutes while stirring; cool the reaction solution to 80°C, and uniformly mix the remaining mixed total alcohol within 30 minutes Add the alcohol into the reaction solution while stirring; continue to feed sulfur dioxide gas under the stirring condition to completely reduce the hexavalent chromium in the solution to trivalent chromium, that is, the chrome tanning solution can not change the color of the acid starch potassium iodide; after the reduction is completed, stir while Add benzoic acid so that the ratio of chromium trioxide to benzoic acid in the solution is 1:0.3, then stir and react at 60°C for 3 hours, and spray dry to obtain a non-pickling chrome tanning a...
Embodiment 2
[0037] After dissolving a certain amount of potassium dichromate in water, add sulfuric acid to make the ratio of the amount of chromium trioxide and sulfuric acid in the solution to be 1:1.5; As a reducing agent, add 80% of the alcohol into the acidic potassium dichromate solution evenly within 60 minutes while stirring; cool the reaction solution to 50°C, and stir the remaining alcohol evenly within 60 minutes While adding to the reaction solution; continue to pass in sulfur dioxide gas under stirring conditions to completely reduce the hexavalent chromium in the solution to trivalent chromium, that is, the chrome tanning solution can not change the color of acid starch potassium iodide; after the reduction is completed, add benzene di Formic acid, so that the ratio of chromium trioxide and phthalic acid in the solution is 1:0.8, then stirred and reacted at 60°C for 0.5h, and spray-dried to obtain a non-pickling chrome tanning agent.
Embodiment 3
[0039] After dissolving a certain amount of potassium dichromate in water, add sulfuric acid so that the ratio of the amount of chromium trioxide and sulfuric acid in the solution is 1:1.8; Mix ethylene glycol evenly, and add 60% of the total alcohol content into the acidic potassium dichromate solution evenly within 30 minutes while stirring; cool the reaction solution to 60°C, and uniformly dissolve the remaining Add the mixed total alcohol into the reaction solution while stirring; continue to feed sulfur dioxide gas under the stirring condition, and completely reduce the hexavalent chromium in the solution to trivalent chromium, that is, the chrome tanning solution cannot change the color of the acid starch potassium iodide; after the reduction is completed, Add naphthalenesulfonic acid while stirring, so that the ratio of chromium trioxide to naphthalenesulfonic acid in the solution is 1:3, then stir and react at 51°C for 4 hours, and spray dry to obtain non-pickling chrom...