[0027] This embodiment provides a composition for resisting dentin sensitivity and preventing dental caries, comprising the following components in parts by weight: 0.1 to 1.5 parts of sodium fluoride, 3 to 7 parts of calcium sodium phosphosilicate, casein phosphopeptide-no 5-20 parts of stereotyped calcium phosphate, 50-80 parts of glycerin.
[0028] In the composition provided in this example, glycerin is used as a solvent to prevent moisture from escaping from the paste, and at the same time increase the cold resistance of the paste. The product is stable in nature, non-toxic and non-corrosive, and is widely used in food and cosmetics; Ions can penetrate into the dentin and combine with calcium salts to form fluorapatite to seal the dentin tubules or reduce the diameter of the dentin tubules, thereby alleviating dentin sensitivity; calcium sodium phosphosilicate reacts with water and saliva, Ion exchange occurs within one minute, continuously releasing calcium and phosphate...
Embodiment 2
[0031] This example provides a composition for resisting dentin sensitivity and preventing dental caries, including the following components in parts by weight: 1.0 parts of sodium fluoride, 5 parts of calcium sodium phosphosilicate, 15 parts of casein phosphopolypeptide-amorphous calcium phosphate parts, 70 parts of glycerin.
Embodiment 3
[0033] The present embodiment provides a preparation method of calcium sodium phosphosilicate as follows: take SiO by weight 2 40~50 parts, CaO15~25 parts, K 2 O 1~30 parts and P 2 o 5 4-6 parts, mix all the components and put them at 1400-1500°C for 60-90 minutes to get a uniform mixture, place the mixture in a normal temperature water bath to quench it, dry it and grind it to the particle size The particles of 10-50nm can obtain the calcium sodium phosphosilicate.