Deodorant for household garbage and preparation method thereof
A technology for household garbage and deodorants, applied in separation methods, chemical instruments and methods, and other chemical processes, can solve problems such as low deodorization efficiency and affect work efficiency, and achieve good masking of odors, reduction of treatment costs, and source wide range of effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example 1
[0031] Preparation example 1 of ore adsorbent: 1. take medical stone powder, zeolite powder and diatomaceous earth with a weight ratio of 3:1:1, ball mill for 4h, and dry through a 200 mesh sieve to obtain ore powder; Heating at a temperature of 400°C for 20 minutes, and then roasting at a temperature of 800°C for 6 hours to obtain roasted ore powder;
[0032] ② Take 30kg of bamboo vinegar, 5kg of tea saponin, 4kg of polyvinyl alcohol, 2kg of ferric chloride and 100kg of water, and mix them evenly to obtain a modifier;
[0033] ③Take 50kg of roasted ore powder, add modifier, stir for 10min at a high speed, then depressurize to -0.09MPa, maintain for 3h, then dry at 80°C for 12h, and pass through a 200-mesh sieve to obtain the ore adsorbent.
preparation example 2
[0034] Preparation example 2 of ore adsorbent: 1. take medical stone powder, zeolite powder and diatomaceous earth with a weight ratio of 3:1:1, ball mill for 5h, and dry through a 200 mesh sieve to obtain ore powder; Heating at a temperature of 450°C for 25 minutes, and then roasting at a temperature of 850°C for 7 hours to obtain roasted ore powder;
[0035] ② Take 35kg of bamboo vinegar, 6kg of tea saponin, 5kg of polyvinyl alcohol, 3kg of ferric chloride and 100kg of water, and mix them evenly to obtain a modifier;
[0036] ③Take 50kg of roasted ore powder, add modifier, stir for 15min at a high speed, then depressurize to -0.09MPa, maintain for 4h, then dry at 85°C for 18h, and pass through a 200-mesh sieve to obtain the ore adsorbent.
preparation example 3
[0037]Preparation example 3 of ore adsorbent: 1. take medical stone powder, zeolite powder and diatomaceous earth with a weight ratio of 3:1:1, ball mill for 6 hours, and dry through a 200 mesh sieve to obtain ore powder; Heating at a temperature of 500°C for 30 minutes, and then roasting at a temperature of 900°C for 8 hours to obtain roasted ore powder;
[0038] ② Take 40kg of bamboo vinegar, 7kg of tea saponin, 6kg of polyvinyl alcohol, 4kg of ferric chloride and 100kg of water, and mix them evenly to obtain a modifier;
[0039] ③Take 50kg of roasted ore powder, add a modifier, stir at a speed of -20min, then depressurize to -0.09MPa, maintain for 5h, then dry at 90°C for 24h, pass through a 200-mesh sieve to obtain an ore adsorbent.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com