Cooling and filtering material and preparation method and application thereof
A technology of filter material and filter section, applied in the field of cooling filter material and its preparation, can solve the problems of limited length space of cooling material, reduce the saturation of smoke aroma, breakage of polylactic acid film, etc., so as to improve the smoking experience and enhance the aroma Effect of saturation, filter performance reduction
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0038] (1) The bleached softwood pulp is beaten with a PFI beater to obtain the bleached softwood pulp with a beating degree of 40 ° SR, and then stirred and dispersed to obtain a bleached softwood pulp dispersion;
[0039] (2) PLA fibers (U.S. NatureWorks) with a fiber length of 6 mm were stirred and dispersed to obtain a PLA fiber dispersion;
[0040] (3) The bleached softwood pulp dispersion obtained in step (1) and the PLA fiber dispersion obtained in step (2) are mixed uniformly in a ratio of 5:5 (dry mass) and then papered on a Fourdrinier paper machine to form quantitative 30g / m 2 paper to obtain coniferous wood pulp / PLA fiber composite cooling filter paper;
[0041] (4) Use a calender to calender the coniferous wood pulp / PLA fiber composite cooling filter paper obtained in step (3) (calendering temperature is 320°C, calendering line pressure: 300kN / m), to obtain coniferous wood pulp / PLA fiber Composite cooling filter material.
Embodiment 2
[0043] (1) The bleached hemp pulp is beaten with a PFI beater to obtain a beating degree of bleached hemp pulp of 45 ° SR, then stirred and dispersed to obtain a bleached hemp pulp dispersion;
[0044] (2) PLA fiber (U.S. NatureWorks) with a fiber length of 4 mm was stirred and dispersed to obtain a PLA fiber dispersion;
[0045] (3) the bleached hemp pulp dispersion that step (1) obtains and the PLA fiber dispersion that step (2) obtains are mixed evenly in the ratio of 4:6 (dry mass) and then carried out on the fourdrinier paper machine and form quantitatively as 120g / m 2 paper to obtain hemp pulp / PLA fiber composite cooling filter paper;
[0046] (4) Use a calender to calender the hemp pulp / PLA fiber composite cooling filter paper obtained in step (3) (calendering temperature is 280°C, calendering line pressure: 280kN / m), and obtain the hemp pulp / PLA fiber composite cooling filter paper filter material.
Embodiment 3
[0048] (1) the bleached bamboo pulp is beaten with a PFI beater to obtain the bleached bamboo pulp with a beating degree of 48 ° SR, then stirred and dispersed to obtain the bleached bamboo pulp dispersion;
[0049](2) PLA fibers (U.S. NatureWorks) with a fiber length of 5 mm were stirred and dispersed to obtain a PLA fiber dispersion;
[0050] (3) the bleached bamboo pulp dispersion liquid that step (1) obtains and the PLA fiber dispersion liquid that step (2) obtains are mixed homogeneously in the ratio of 3:7 (dry mass) after papering on the fourdrinier paper machine and form quantitatively as 240g / m 2 paper to obtain bamboo pulp / PLA fiber composite cooling filter paper;
[0051] (4) Using a calender to calender the bamboo pulp / PLA fiber composite cooling filter paper obtained in step (3) (calendering temperature is 250°C, calendering line pressure: 260kN / m), to obtain bamboo pulp / PLA fiber composite cooling filter material.
PUM
Property | Measurement | Unit |
---|---|---|
length | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com