Embodiment 1
[0115] 1) Preparation of emulsified acid-acid phase: get 97.0 parts by mass concentration of 15wt% hydrochloric acid aqueous solution, at a stirring speed of 500r / min, add 1.0 parts by mass of iron ion stabilizer ethylenediaminetetraacetic acid ( Commercially available) and 2.0 parts by mass of 1-aminoethyl-2-pentadecyl imidazoline quaternary ammonium corrosion inhibitor, then, stirred for 1 hour at a stirring speed of 500r / min;
[0116] 2) Preparation of emulsified acid oil phase: 2.0 parts by mass of dipolyhydroxystearate and 0.5 part by mass of hexadecylamine were heated to 50°C and dissolved in 97.5 parts by mass of diesel oil, and stirred evenly at a stirring speed of 500 r / min. Cool to natural ambient temperature;
[0117] 3) Preparation of emulsified acid: the volume ratio of the acid phase and the oil phase is 75:25, and the acid phase is slowly added dropwise to the oil phase at a rate of 80 drops / min at a stirring speed of 1500r / min, and the Continue to stir 20min u...
Embodiment 2
[0121] 1) Preparation of emulsified acid-acid phase: get 96.5 parts by mass concentration of 15wt% hydrochloric acid aqueous solution, add 1.2 parts by mass of iron ion stabilizer citric acid (commercially available) and 2.3 parts by mass of 2-methylquinoline benzyl quaternary ammonium salt corrosion inhibitor (commercially available), then stirred for 0.5 hour at a stirring speed of 1500r / min;
[0122] 2) Preparation of emulsified acid oil phase: 1.5 parts by mass of sorbitan sesquioleate and 0.5 parts by mass of polyoxyethylene octylphenol ether-10 were heated to 40°C and dissolved in 98 parts by mass of white oil. Stir evenly at a stirring speed of min, and cool to natural ambient temperature;
[0123] 3) Preparation of emulsified acid: the volume ratio of the acid phase and the oil phase is 65:35, and the acid phase is slowly added dropwise to the oil phase at a rate of 60 drops / min under the condition of a stirring speed of 2000 r / min, and the Continue stirring for 15min...
Embodiment 3
[0127] 1) Preparation of emulsified acid phase: get 96.0 parts by mass concentration of 20wt% hydrochloric acid aqueous solution, add 1.5 parts by mass of iron ion stabilizer (acetic acid and citric acid with 1 : 1 mass ratio mixed mixture) and 2.5 mass parts formaldehyde-p-phenylenediamine-acetophenone corrosion inhibitor (commercially available), then, stirred 2 hours at 1000r / min stirring speed;
[0128] 2) Preparation of emulsified acid oil phase: 2.0 parts by mass of sorbitan fatty acid ester and 2 parts by mass of polyoxyethylene octylphenol ether-10 were heated to 60°C and dissolved in 96 parts by mass of light crude oil, and Stir evenly at a stirring speed of 1000r / min, and cool to natural ambient temperature;
[0129] 3) Preparation of emulsified acid: the volume ratio of the acid phase and the oil phase is 60:40, under the condition of a stirring speed of 2500r / min, the acid phase is slowly added dropwise to the oil phase at a speed of 120 drops / min, dropwise Contin...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com