Environment-friendly antibacterial polypropylene material special for sprayers and preparation method of material
An antibacterial polypropylene and sprayer technology, applied in the field of polypropylene materials, can solve the problems of low transparency, low rigidity, easy residual liquid materials, etc., and achieve the effect of rapid recovery
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] An environmentally friendly and antibacterial polypropylene material for sprayers, comprising:
[0028]The weight part is the wood pulp fiber treatment material of 40 parts, and described wood pulp fiber treatment material comprises colloid binder, wood pulp fiber and quartz sand, and its percentage by weight is colloid binder 20%, wood pulp fiber 45% and Quartz sand 22%; And, the preparation method of wood pulp fiber treatment material is to add the wood pulp fiber to vibrate, then the quartz sand is scattered and sprinkled on the wood pulp fiber, increases vibration frequency, finally adds colloidal binder, After shaking for 10 minutes, let it stand still for 1-3 hours;
[0029] Parts by weight are 15 parts of dispersants;
[0030] Parts by weight are 5 parts of antioxidants;
[0031] Parts by weight are 18 parts of rubber, wherein protein is added in the rubber, wherein the mass ratio of protein to rubber added is 3:89;
[0032] The weight part is 80 parts of poly...
Embodiment 2
[0042] An environmentally friendly and antibacterial polypropylene material for sprayers, comprising:
[0043] The weight part is the wood pulp fiber treatment material of 70 parts, and described wood pulp fiber treatment material comprises colloid binder, wood pulp fiber and quartz sand, and its percentage by weight is colloid binder 29%, wood pulp fiber 58% and Quartz sand 30%; And, the preparation method of wood pulp fiber treatment material is to shake the added wood pulp fiber, then spread the quartz sand on the wood pulp fiber, increase the vibration frequency, and finally add colloidal binder, After shaking for 30 minutes, let it stand for 3 hours;
[0044] Parts by weight are 27 parts of dispersants;
[0045] The weight part is the antioxidant of 9 parts;
[0046] Parts by weight are 28 parts of rubber, wherein protein is added in the rubber, wherein the mass ratio of protein to rubber is 8:100;
[0047] The weight part is 120 parts of polypropylene base material, a...
Embodiment 3
[0057] An environmentally friendly and antibacterial polypropylene material for sprayers, comprising:
[0058] The weight portion is the wood pulp fiber treatment material of 56 parts, and described wood pulp fiber treatment material comprises colloid binder, wood pulp fiber and quartz sand, and its percentage by weight is colloid binder 29%, wood pulp fiber 58% and Quartz sand 30%; And, the preparation method of wood pulp fiber treatment material is to shake the added wood pulp fiber, then spread the quartz sand on the wood pulp fiber, increase the vibration frequency, and finally add colloidal binder, After shaking for 30 minutes, let it stand for 3 hours;
[0059] Parts by weight are 21 parts of dispersants;
[0060] Parts by weight are 7 parts of antioxidants;
[0061] Parts by weight are 23 parts of rubber, wherein protein is added in the rubber, wherein the mass ratio of protein to rubber is 4:95;
[0062] The weight part is 97 parts of polypropylene primer, which is ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com