A kind of sewage treatment agent, the technology of mass parts, applied in the direction of water/sewage treatment, adsorption water/sewage treatment, water/sludge/sewage treatment, etc., can solve the problems of difficult separation and recovery of photocatalysts, loss and waste, etc., to achieve improved catalytic performance performance, avoid loss and waste, and the effect of many pores
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0031] The present embodiment provides a kind of preparation method of sewage treatment agent, comprises the following steps:
[0032] Step 1, mix 80 grams of dimethyl diallyl ammonium chloride, 80 grams of acrylamide, 6 grams of ethylenediamine tetraacetic acid, 4 grams of polyethylene glycol, 10 grams of fatty amine, 20 grams of hydroxypropyl methylcellulose Add plain sodium and 20 grams of water into the reaction kettle, mix and stir for 4 hours at a temperature of 40° C. to obtain the first mixture;
[0033] Step 2, mixing and stirring 240 grams of polyaluminum chloride, 180 grams of polyacrylamide, 20 grams of zinc oxide, 20 grams of bentonite and 50 grams of water at a temperature of 40° C. for 1 hour to obtain a second mixture;
[0034] Step 3, mixing and stirring the first mixture obtained in step 1 and the second mixture obtained in step 2 to obtain a modified polyacrylamide;
[0035] Step 4, mixing and stirring 10 grams of sodium pyrophosphate, 60 grams of titanium ...
Embodiment 2
[0041] The present embodiment provides a kind of preparation method of sewage treatment agent, comprises the following steps:
[0042] Step 1, 100 grams of dimethyl diallyl ammonium chloride, 120 grams of acrylamide, 10 grams of ethylenediaminetetraacetic acid, 12 grams of polyethylene glycol, 20 grams of fatty amine, 60 grams of hydroxypropyl methylcellulose Add plain sodium and 20 grams of water into the reaction kettle, mix and stir for 2 hours at a temperature of 50° C. to obtain the first mixture;
[0043] Step 2, mixing and stirring 320 grams of polyaluminum chloride, 240 grams of polyacrylamide, 60 grams of zinc oxide, 60 grams of bentonite and 50 grams of water at a temperature of 50°C for 0.5 hours to obtain a second mixture;
[0044] Step 3, mixing and stirring the first mixture obtained in step 1 and the second mixture obtained in step 2 to obtain a modified polyacrylamide;
[0045] Step 4, mixing and stirring 20 grams of sodium pyrophosphate, 100 grams of titanium...
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com