Piston rod lug ring welding process
A welding process and piston rod technology, applied in the field of piston rods, can solve problems such as low welding efficiency and unstable welding quality of friction welding, achieve high heating efficiency, increase welding efficiency, and reduce metal embrittlement
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] A piston rod earring welding process, comprising the following steps:
[0020] S1 Piston rod end and piston rod earring are cleaned, the piston rod end and piston rod earring are cleaned with metal cleaning agent, and the metal cleaning agent includes deionized water, silicone oil, sodium stearate, sodium phosphate, methyl Silane, distearyl dimethyl ammonium chloride, octanol, the mass ratio of the above components is 15-30 parts: 1-2 parts: 10-20 parts: 10-20 parts: 0.5-1 parts: 3-8 Servings: 0.5-1 serving;
[0021] S2 The cleaned piston rod tail and the piston rod earring are fixed on the equipment, the piston rod tail is set on the rotating device, and the piston rod earring is set on the mobile pressurizing device. The mobile pressurizing device cannot be rotated but can be pressurized movement;
[0022] S3 The piston rod tail and the piston rod earring are preheated. The piston rod tail and the piston rod earring body are heated by infrared, and the heating tempe...
Embodiment 2
[0027] The difference between this embodiment and Embodiment 1 is that the heating temperature of the piston rod and the piston rod earring is different.
[0028] A piston rod earring welding process, comprising the following steps:
[0029] S1 Piston rod end and piston rod earring are cleaned, the piston rod end and piston rod earring are cleaned with metal cleaning agent, and the metal cleaning agent includes deionized water, silicone oil, sodium stearate, sodium phosphate, methyl Silane, distearyl dimethyl ammonium chloride, octanol, the mass ratio of the above components is 15-30 parts: 1-2 parts: 10-20 parts: 10-20 parts: 0.5-1 parts: 3-8 Servings: 0.5-1 serving;
[0030] S2 The cleaned piston rod tail and the piston rod earring are fixed on the equipment, the piston rod tail is set on the rotating device, and the piston rod earring is set on the mobile pressurizing device. The mobile pressurizing device cannot be rotated but can be pressurized movement;
[0031] S3 Th...
Embodiment 3
[0036] The difference between this embodiment and Embodiment 1 is that the rotation speed of the rotating equipment in step S4 is different.
[0037] A piston rod earring welding process, comprising the following steps:
[0038] S1 Piston rod end and piston rod earring are cleaned, the piston rod end and piston rod earring are cleaned with metal cleaning agent, and the metal cleaning agent includes deionized water, silicone oil, sodium stearate, sodium phosphate, methyl Silane, distearyl dimethyl ammonium chloride, octanol, the mass ratio of the above components is 15-30 parts: 1-2 parts: 10-20 parts: 10-20 parts: 0.5-1 parts: 3-8 Servings: 0.5-1 serving;
[0039] S2 The cleaned piston rod tail and the piston rod earring are fixed on the equipment, the piston rod tail is set on the rotating device, and the piston rod earring is set on the mobile pressurizing device. The mobile pressurizing device cannot be rotated but can be pressurized movement;
[0040] S3 The piston rod ...