A soil conditioner and a technology for saline-alkali land, which are applied in the field of a special soil conditioner for medium and mild saline-alkali land and its preparation field, can solve the problems of inability to meet the needs of agricultural planting, single function, and inability to fundamentally change the growing environment of crops.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0036] A special soil conditioner for mild to moderate saline-alkali land, calculated in parts by weight, comprising the following components:
[0037] 65 parts of modified phosphogypsum powder, 15 parts of sulfur powder, 3 parts of soil humic acid, 4 parts of fulvic acid and 14 parts of calcium lignosulfonate.
[0038] The particle size of the modified phosphogypsum powder is 150-180 μm.
[0039] The preparation method of modified phosphogypsum powder is:
[0040] Step 1, prepare gypsum powder crystal phase transformation product:
[0041]S1. Weigh phosphogypsum powder and place it in a sulfuric acid solution with a mass fraction of 10% to 20%, heat up to 65 to 75°C, stir for 2 to 3 hours, filter and wash the collected solid product with distilled water until the washing liquid is Neutral, and then placed in an oven at 100 ° C to dry to obtain a pre-treatment of phosphogypsum powder; wherein, the mass ratio of phosphogypsum powder and sulfuric acid solution is 1:8;
[0042...
Embodiment 2
[0050] A special soil conditioner for mild to moderate saline-alkali land, calculated in parts by weight, comprising the following components:
[0051] 45 parts of modified phosphogypsum powder, 12 parts of sulfur powder, 1 part of water humic acid, 2 parts of fulvic acid and 10 parts of calcium lignosulfonate.
[0052] The particle size of the modified phosphogypsum powder is 150-180 μm.
[0053] The preparation method of modified phosphogypsum powder is:
[0054] Step 1, prepare gypsum powder crystal phase transformation product:
[0055] S1. Weigh phosphogypsum powder and place it in a sulfuric acid solution with a mass fraction of 10% to 20%, heat up to 65 to 75°C, stir for 2 to 3 hours, filter and wash the collected solid product with distilled water until the washing liquid is Neutral, and then placed in an oven at 100 ° C to dry to obtain a pre-treatment of phosphogypsum powder; wherein, the mass ratio of phosphogypsum powder and sulfuric acid solution is 1:10;
[00...
Embodiment 3
[0064] A special soil conditioner for mild to moderate saline-alkali land, calculated in parts by weight, comprising the following components:
[0065] 78 parts of modified phosphogypsum powder, 18 parts of sulfur powder, 8 parts of mold humic acid, 5 parts of fulvic acid and 20 parts of calcium lignosulfonate.
[0066] The particle size of the modified phosphogypsum powder is 150-180 μm.
[0067] The preparation method of modified phosphogypsum powder is:
[0068] Step 1, prepare gypsum powder crystal phase transformation product:
[0069] S1. Weigh phosphogypsum powder and place it in a sulfuric acid solution with a mass fraction of 10% to 20%, heat up to 65 to 75°C, stir for 2 to 3 hours, filter and wash the collected solid product with distilled water until the washing liquid is Neutral, and then placed in a 100 ℃ oven to dry to obtain a pre-treatment of phosphogypsum powder; wherein, the mass ratio of phosphogypsum powder and sulfuric acid solution is 1:5;
[0070] S2....
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle diameter | aaaaa | aaaaa |
| particle size (mesh) | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More