Graphene oxide-pyraclostrobin nano-suspension concentrate, preparation method and application thereof
A technology of pyraclostrobin and nano-suspension, which is applied in chemical instruments and methods, botany equipment and methods, applications, etc., and can solve problems such as endangering non-target biological safety
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] Weigh the following materials in proportion: active ingredient 32%, maleic acid acrylic acid copolymer sodium salt 2%, emulsifier 6%, ethylene glycol 5%, xanthan gum 0.1%, Cathone 0.2%, ethoxylated silicone oil 0.3 %, balance water;
[0033] The mass ratio of styrylphenol polyoxyethylene ether to tristyrylphenol polyoxyethylene ether phosphate in the emulsifier is 2:1. The emulsifier is a mixture of styrylphenol polyoxyethylene ether and tristyrylphenol polyoxyethylene ether phosphate.
[0034] Composite graphene oxide and pyraclostrobin according to the above ratio, then add maleic acid acrylic acid copolymer sodium salt, emulsifier, ethylene glycol, Cathone, organosilicon compound and water, stir to obtain a mixture, Colloidal milling first, and then grinding to a qualified particle size by a sand mill, and finally pouring into a high-speed mixer, and adding thickener xanthan gum to obtain graphene oxide-pyraclostrobin nano-suspension.
[0035] The mass ratios of gr...
Embodiment 2
[0040] Weigh the following materials in proportion: 35% active ingredient, 3% sodium salt of maleic acid acrylic acid copolymer, 9% emulsifier, 4% ethylene glycol, 0.05% xanthan gum, 0.1% Cathone, 0.2% ethoxylated silicone oil %, balance water;
[0041] The mass ratio of styrylphenol polyoxyethylene ether to tristyrylphenol polyoxyethylene ether phosphate in the emulsifier is 2:1. The emulsifier is a mixture of styrylphenol polyoxyethylene ether and tristyrylphenol polyoxyethylene ether phosphate.
[0042] The mass ratio of graphene oxide and pyraclostrobin in the active ingredient is 5:5.
[0043] The preparation method is the same as in Example 1.
Embodiment 3
[0045] Weigh the following materials in proportion: active ingredient 30%, maleic acid acrylic acid copolymer sodium salt 1%, emulsifier 3%, ethylene glycol 6%, xanthan gum 0.15%, Cathone 0.3%, ethoxylated silicone oil 0.4 %, balance water;
[0046] The mass ratio of styrylphenol polyoxyethylene ether to tristyrylphenol polyoxyethylene ether phosphate in the emulsifier is 2:1. The emulsifier is a mixture of styrylphenol polyoxyethylene ether and tristyrylphenol polyoxyethylene ether phosphate.
[0047] The mass ratio of graphene oxide and pyraclostrobin in the active ingredient is 5:5.
[0048] The preparation method is the same as in Example 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com