Preparation method of antibacterial polypropylene fiber yarn capable of releasing negative ions and prepared polypropylene fiber carpet
An anion, polypropylene technology, applied in the manufacture of rayon, single-component polyolefin rayon, fiber chemical characteristics, etc., can solve problems such as undescribed, and achieve no special additives, high anion release, and simple process. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0029] A kind of preparation method of releasing the antibacterial polypropylene fiber yarn of negative ion comprises the steps:
[0030] Step 1, surface modification treatment of tourmaline powder particles.
[0031] Tourmaline powder belongs to natural mineral materials. It is a silicate mineral with a complex ring structure characterized by boron content (edited by Tian Junying, Yang Wenfang, Niu Jiarong, etc., "Functional Finishing of Textiles", China Textile Publishing Society, 2015.10). After grinding, the particle size is reduced. The tourmaline powder selected in the present invention includes manganese tourmaline powder, ferrotourmaline powder, lithium tourmaline powder and magnesium tourmaline powder. 6000-mesh powder is preferred, and 10000-mesh powder and 12000-mesh powder are more preferred.
[0032] Tourmaline is a natural mineral material with a Mohs hardness of 7-7.5, which is harder than steel, teeth, and quartz. The harder the material, the more difficult...
Embodiment 1
[0048] Example 1: Preparation of antibacterial polypropylene yarn releasing negative ions with a tourmaline powder content of 0.4% and the resulting carpet.
[0049] Step 1, surface modification treatment of tourmaline powder particles;
[0050] (1) Mix the tourmaline powder particles and the interface compatibilizer uniformly at room temperature.
[0051] Weigh the tourmaline powder and the interface compatibilizer, and mix them evenly in the mixing equipment. Mixing equipment speed: 100 rpm. Mixing time: 20 minutes. The absolute dry mass ratio of tourmaline powder to interface compatibilizer is 95:5. Thus, a normal-temperature mixture of tourmaline powder particles and an interface compatibilizer is obtained. Among them, the tourmaline powder is: 12000 mesh iron tourmaline powder particles. The interface compatibilizer is a mixture of hydroxyethyl ethylene bis stearamide and liquid paraffin (distillation temperature > 300° C.) according to the dry mass ratio of 4:1.
...
Embodiment 2
[0056] Embodiment 2: Preparation of antibacterial polypropylene yarn releasing negative ions with 1.0% tourmaline powder content and the carpet obtained.
[0057] Step 1, surface modification treatment of tourmaline powder particles;
[0058] (1) Mix the tourmaline powder particles and the interface compatibilizer uniformly at room temperature. Weigh the tourmaline powder and the interface compatibilizer, and mix them evenly in the mixing equipment. Mixing equipment speed: 100 rpm. Mixing time: 20 minutes. The dry mass ratio of tourmaline powder to interface compatibilizer is 90:10. Thus, a normal-temperature mixture of tourmaline powder particles and an interface compatibilizer is obtained. Among them, the tourmaline powder is: 10000 mesh iron tourmaline powder particles. The interface compatibilizer is a mixture of hydroxyethyl ethylene bis stearamide, polyethylene wax and liquid paraffin (distillation temperature > 300° C.) according to the dry mass ratio of 7:2:1.
...