Supporting material for building permeable reactive barrier and application of supporting material
A technology of reaction wall and construction method, applied in soil protection, construction, excavation, etc., can solve the problems of poor ditch wall support ability, easy collapse, loss of part or all of the pollutant repair ability, etc. The effect of uniform molding and production cost reduction
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0050] This embodiment provides a support material, including a first component and a second component;
[0051] The first component comprises guar gum, xanthan gum, sodium bicarbonate and datamone with a mass ratio of 54:36:8:2, and the preparation method of the first component comprises, combining guar gum, xanthan gum , sodium bicarbonate and datamon were mixed evenly, added to water, and mixed evenly to obtain the first component whose concentration was 2g / L.
[0052] The second component includes mannanase, and the mannanase is dissolved in water at 0.5 g / L to obtain the second component.
Embodiment 2
[0054] This embodiment provides a support material, including a first component and a second component;
[0055] The first component comprises guar gum, xanthan gum, mannan, sodium bicarbonate and azoxystrobin with a mass ratio of 59.5:17:8.5:13:2, and the preparation method of the first component comprises: Yeldou gum, xanthan gum, mannan, sodium bicarbonate and azoxystrobin were mixed uniformly, added to water, and mixed uniformly to obtain the first component with a concentration of 5 g / L.
[0056] The second component includes galactomannanase and mannanase with a mass ratio of 80:20, and galactomannanase and mannanase are dissolved in water to obtain a concentration of the second group of 2g / L point.
Embodiment 3
[0058] This embodiment provides a support material, including a first component and a second component;
[0059] The first component comprises guar gum, gum arabic, xanthan gum, sodium hydroxide and chlorobromoisocyanuric acid with a mass ratio of 57:28.5:8.5:5:1, and the preparation method of the first component comprises, Guar gum, gum arabic, xanthan gum, sodium hydroxide and chlorobromoisocyanuric acid were mixed uniformly, added to water, and mixed uniformly to obtain the first component with a concentration of 7 g / L.
[0060] The second component includes galactomannanase and rhamnosidase with a mass ratio of 75:25, and galactomannanase and rhamnosidase are dissolved in water to obtain a concentration of 3g / L for the second group point.
PUM
Property | Measurement | Unit |
---|---|---|
concentration | aaaaa | aaaaa |
quality score | aaaaa | aaaaa |
quality score | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com