Unsaturated polyester resin material for glass fiber reinforced plastic pipeline and preparation method of unsaturated polyester resin material
A polyester resin and unsaturated technology is applied in the field of unsaturated polyester resin materials for glass fiber reinforced plastic pipes and their preparation, which can solve the problems of affecting the quality of continuously wound glass fiber reinforced plastic pipes, unable to fully utilize continuous winding equipment, and poor mechanical properties of pipes, etc. To achieve the effect of facilitating continuous winding, improving elasticity, and improving interface bonding strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0026] The preparation method of the unsaturated polyester resin material for FRP pipes of the present invention comprises the following steps:
[0027] (1) Mix the unsaturated polyester resin base material with the natural latex and stir quickly, then add the flame retardant, stir for 1-2 hours, and finally add styrene and stir evenly to obtain a resin mixture;
[0028] (2) adding the ionic liquid modified carbon fiber and the curing accelerator into the resin mixture of step (1), stirring and mixing to obtain the mixture;
[0029] (3) Pour the mixture of step (2) into the material trough of the winding machine, add modified waste circuit board powder, thixotropic agent and curing agent, and enter the mold for high temperature curing through the weaving and winding pultrusion process of the winding machine. Forming, cooling to room temperature to obtain unsaturated polyester resin material for glass fiber reinforced plastic pipes.
[0030] The raw materials of the modified w...
Embodiment 1
[0038] The raw materials of the modified waste circuit board powder in this embodiment, in terms of mass percentage, include 60% waste circuit board powder, 40% vinyltriethoxysilane and an aqueous ethanol solution.
[0039] The preparation method of the modified waste circuit board powder comprises the following steps:
[0040] (1) vinyltriethoxysilane is added to the ethanol aqueous solution, heat up and stir rapidly to obtain mixed modified liquid;
[0041] (2) adding the waste circuit board powder to the mixed modification solution of step (1), heating up and stirring for 2 hours, filtering, washing the filter residue with deionized water 3 times, and drying to obtain the modified waste circuit board powder.
Embodiment 2
[0043] The raw materials of the modified waste circuit board powder in this embodiment, in terms of mass percentage, include 70% waste circuit board powder, 30% vinyltrimethoxysilane and an aqueous ethanol solution.
[0044]The preparation method of the modified waste circuit board powder comprises the following steps:
[0045] (1) vinyltrimethoxysilane is added to the ethanol aqueous solution, heats up and stirs rapidly to obtain a mixed modified liquid;
[0046] (2) adding the waste circuit board powder to the mixed modification solution of step (1), heating up and stirring for 4h, filtering, washing the filter residue with deionized water 4 times, and drying to obtain the modified waste circuit board powder
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More