Coal energy-saving clean proliferating agent
A value-added agent and clean technology, which is applied in the field of carbon-burning energy-saving clean value-added agents, can solve the problems of poor comprehensive effect, inconvenient storage, unsatisfactory desulfurization effect, etc., and achieve quick results, simple production process, and rich raw materials.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] Embodiment one: Type A value-added agent:
[0016] Oil shale 68-81%, humic acid 10-15%, acidified gangue 2-6%, sodium nitrate 3-10%, potassium permanganate 1-5%, aluminum sulfate 3-6%, sodium chloride 3 -10%, calcium carbonate 5-10%, sodium carbonate 2-8%, manganese dioxide 3-7%, sodium phosphate 3-5%, light magnesium oxide 5-10%.
[0017] The raw materials of the above components are mixed and pulverized according to the percentage weight, and the powder fineness is 20-40 mesh, and then put into the mixer and stirred for 5-10 minutes, and the finished product is inspected and packaged.
[0018] This type A value-added agent is suitable for burning coal with a volatile content of 2.5-3.5%, a calorific value of 3500-4500 kcal / kg, and a sulfur content of 1.2%. The dosage is 1% of that of coal.
Embodiment 2
[0019] Embodiment two: B type value-added agent:
[0020] Oil shale 40-68%, humic acid 11-14%, acidified gangue 2-5%, sodium nitrate 4-10%, potassium permanganate 1-3%, aluminum sulfate 4-5%, sodium chloride 3% -8%, calcium carbonate 6-8%, sodium carbonate 2-5%, manganese dioxide 3-6%, sodium phosphate 3-5%, light magnesium oxide 6-8%.
[0021] The raw materials of the above components are mixed and pulverized with a pulverizer, and the powder fineness is 20-40 mesh, and then put into a mixer and stirred for 5-10 minutes, fully mixed evenly, and then packaged as a finished product.
[0022] This B-type filler is suitable for coal-fired with volatile content of 3.5-4.5%, calorific value of 4500-5500 kcal / kg, and sulfur content of less than 1.5%. The dosage is 1.5% of coal-fired.
Embodiment 3
[0023] Embodiment three: Type C value-added agent:
[0024] Oil shale 40-58%, humic acid 10-12%, acidified coal gangue 4-6%, sodium nitrate 4-8%, potassium permanganate 1-2%, aluminum sulfate 5-6%, calcium carbonate 6- 10%, sodium chloride 4-8%, sodium carbonate 2-6%, manganese dioxide 3-6%, sodium phosphate 4-5%, light magnesium oxide 6-8%.
[0025] The raw materials of the above components are mixed and pulverized by a pulverizer until the fineness of the powder reaches 20-40 meshes, and then put into a mixer and stirred for 5-10 minutes, and the mixture is evenly mixed before being packaged as a finished product.
[0026] This C-type filler is suitable for coal-fired coal with a volatile content of 3-6%, a calorific value of 4000-6000 kcal / kg, and a sulfur content below 1.6%, especially for domestic coal-fired use. 1%, this C-type value-added agent has a wide range of applications.
PUM
Property | Measurement | Unit |
---|---|---|
heating value | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com