[0014] First, in a capacity of 1000 liters of enamel reaction kettle, add quantitative water, add the ethylene glycol butyl ether solvent that the weight content is 2%, stir evenly, add the tensio-active agent (perfluorononoxybenzenesulfonate) of weight 1.0% Sodium acid), stirring and dissolving completely, and then adding organic phosphonic acid (hydroxyethylidene diphosphonic acid and phosphinotrialkyltricarboxylic acid) with a weight content of 21.0% in sequence (the compound ratio is 1: 2), and the weight content is 18% The polycarboxylic acid (hydrolyzed polymaleic anhydride), the balance is water, stir evenly, both obtained this product.
[0015] The composite anti-scaling agent is used in anti-scaling construction of scaled oil wells or in cooperation with fracturing and acidification. When used, generally, the dosage of a single well is 2-5 tons, the mass concentration is 2-6%, and the effective period of anti-scaling is more than 2 years.
Embodiment 2
[0017] First in a capacity of 1000 liters of enamel reaction kettle, add quantitative water, add weight content is 2% ethylene glycol butyl ether solvent, stir evenly, add weight 1.2% tensio-active agent (perfluorononoxybenzene sulfonate Sodium acid), stirring and dissolving completely, and then adding organic phosphonic acid (hydroxyethylidene diphosphonic acid and phosphinotrialkyltricarboxylic acid) with a weight content of 24.0% in sequence (the compound ratio is 1: 2), and the weight content is 15% The polycarboxylic acid (maleic acid-acrylic acid copolymer), the balance is water, stirs evenly, both obtains this product.
[0018] The composite anti-scaling agent is used in anti-scaling construction of scaled oil wells or in cooperation with fracturing and acidification. Generally, the dosage for a single well is 2-5 tons, the concentration is 2-6%, and the effective period of anti-scaling is more than 2 years.
Embodiment 3
[0020] First in a capacity of 1000 liters of enamel reaction kettle, add quantitative water, add weight content is 2% ethylene glycol butyl ether solvent, stir evenly, add weight 1.2% tensio-active agent (perfluorononoxybenzene sulfonate Sodium acid sodium), stir and dissolve completely, then add the organic phosphonic acid (aminotrimethylene phosphonic acid) of 20.0% by weight and the polycarboxylic acid (maleic acid-acrylic acid-AMPS copolymer) of 20% by weight successively, the balance For water, stir evenly to obtain the product.
[0021] The composite anti-scaling agent is used in anti-scaling construction of scaled oil wells or in cooperation with fracturing and acidification. Generally, the dosage for a single well is 2-5 tons, the concentration is 2-6%, and the effective period of anti-scaling is more than 2 years.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com