A kind of preparation technology of low-cost environment-friendly interior wall paint
An environmentally friendly coating and preparation process technology, applied in the field of building decoration materials, can solve problems such as high cost, and achieve the effects of low cost, cost reduction, and simple preparation process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A kind of preparation technology of low-cost environment-friendly paint, this technology comprises the steps:
[0022] a. Preparation of straw powder: Wash the plant straw, then bleach it with an appropriate amount of bleaching powder, then wash it with water, then soak it in 12% high-purity zinc oxide aqueous solution for 36 hours, then dry it at 120°C for 12 hours, and finally put the Zinc and dried stalks are pulverized into ultra-fine powder by a pulverizer.
[0023] b. Preparation of mixture: mix 30-40% of the straw powder prepared in step a with 10-15% of calcium carbonate, 10-15% of magnesium carbonate, and 10-15% of bentonite in a ball mill for 8 hours, Prepare a uniform mixture, wherein the content is a percentage by weight, and its content is the ratio of the total weight of the final coating;
[0024] c. prepare the coating: the mixture prepared in step b is mixed with 2-3% hydroxyethyl cellulose, 3-5% white latex and the water of the balance in percentage i...
Embodiment 2
[0026] A kind of preparation technology of low-cost environment-friendly paint, this technology comprises the steps:
[0027] a. Preparation of straw powder: clean the plant straw, then bleach it with an appropriate amount of bleaching powder, then wash it with water, then soak it in 15% high-purity zinc oxide aqueous solution for 60 hours, then dry it at 120-150°C for 18 hours, and finally soak the straw The dried straw with zinc oxide is pulverized into superfine powder by a pulverizer.
[0028] b. Preparation of mixture: mix 30-40% of the straw powder prepared in step a with 10-15% of calcium carbonate, 10-15% of magnesium carbonate, and 10-15% of bentonite in a ball mill for 12 hours, Prepare a uniform mixture, wherein the content is a percentage by weight, and its content is the ratio of the total weight of the final coating;
[0029] c. prepare the coating: the mixture prepared in step b is mixed with 2-3% hydroxyethyl cellulose, 3-5% white latex and the water of the ba...
Embodiment 3
[0031] A kind of preparation technology of low-cost environment-friendly paint, this technology comprises the steps:
[0032] a. Preparation of straw powder: Wash the plant straw, then bleach it with an appropriate amount of bleaching powder, then wash it with water, then soak it in 13% high-purity zinc oxide aqueous solution for 45 hours, then dry it at 135°C for 15 hours, and finally put the Zinc and dried stalks are pulverized into ultra-fine powder by a pulverizer.
[0033] b. Preparation of mixture: mix 30-40% of the straw powder prepared in step a with 10-15% of calcium carbonate, 10-15% of magnesium carbonate, and 10-15% of bentonite in a ball mill for 10 hours, Prepare a uniform mixture, wherein the content is a percentage by weight, and its content is the ratio of the total weight of the final coating;
[0034] c. prepare the coating: the mixture prepared in step b is mixed with 2-3% hydroxyethyl cellulose, 3-5% white latex and the water of the balance in percentage ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com