A technology of aeration device and air layer, which is applied in sustainable biological treatment, water/sludge/sewage treatment, biological water/sewage treatment, etc. It can solve the problems of unfavorable treatment of sewage and single function, and prolong the backwash cycle. , the preparation process is simple and the cost is low
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation Embodiment 1
[0076] This example is used to illustrate the preparation of the coated silica sand provided by the present invention.
[0077] 100 grams of quartz sand particles with a particle size of 70 mesh (224 microns) and a sphericity of 0.8 and quartz sand particles with a particle size of 140 mesh (105 microns) and a sphericity of 0.8 were heated to 50°C, and then, Add 6 grams of liquid polyvinyl alcohol tert-butyraldehyde modified epoxy resin, stir well, then add 1 gram of polyamide curing agent, and stir evenly, so that the epoxy resin is coated on the surface of the quartz sand particles; however, cool to room temperature, break 1. Obtain hydrophobic particles after sieving, and calculate by weight gain method, take the silica sand with polymer coating as a benchmark, and the content of polymer coating is 7% by weight.
preparation Embodiment 2
[0079] This example is used to illustrate the preparation of the coated silica sand provided by the present invention.
[0080] According to the method for embodiment 1, and utilize the raw material as shown in table 1, be 40 orders (450 microns) respectively with 100 grams of particle diameters, the quartz sand particle that sphericity is 0.65 and particle diameter be 70 orders (224 microns) 1. Quartz sand particles with a sphericity of 0.65 are prepared as hydrophobic particles with a polymer coating.
preparation Embodiment 3-8
[0082] This example is used to illustrate the preparation of the coated silica sand provided by the present invention.
[0083] According to the method of embodiment 1, and utilize the raw material as shown in table 1, make hydrophobic particles respectively, wherein, the diameter of the quartz sand particle used in the preparation embodiment 3 is 280 microns, and the diameter of the quartz sand particle in the preparation embodiment 4 is 154 microns, the diameter of the quartz sand particles in Preparation Examples 5 and 6 is 315 microns, the diameter of the quartz sand particles in Preparation Example 7 is 355 microns, and the diameter of the quartz sand particles in Preparation Example 8 is 200 microns.
[0084] Table 1
[0085]
[0086] By weight gain method, calculate the silica sand that the surface that preparation embodiment 2-8 obtains is coated with coating layer, take the silica sand with polymer coating layer as benchmark, the content of polymer coating layer is...
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com