Antistatic finishing agent for wool and wool blended fabrics and preparation method thereof
An antistatic finishing agent, wool technology, applied in fiber treatment, animal fiber, textiles and papermaking, etc., can solve the problems of difficult to widely use, processing and use conditions, etc., to achieve improved soaping resistance, good softness, Effect of Surface Resistance Decrease
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] An antistatic finishing agent for wool and its blended fabrics, in parts by weight, consists of the following components:
[0020] Dimethicone: 2, Polymethylhydrogensiloxane: 1,
[0021] Butyl Acrylate: 10, Methyl Nepal: 1, Glycerin: 10,
[0022] Potassium Alkylbenzene Sulfonate: 0.2, Hydroxypropyl Acrylate: 3,
[0023] Calcium Chloride: 2, Macrogol Stearate: 5, Water: 80.
Embodiment 2
[0025] An antistatic finishing agent for wool and its blended fabrics, in parts by weight, consists of the following components:
[0026] Dimethicone: 5, Polymethylhydrogensiloxane: 3,
[0027] Butyl Acrylate: 20, Methyl Nepal: 3, Glycerin: 20,
[0028] Potassium Alkylbenzene Sulfonate: 0.6, Hydroxypropyl Acrylate: 8,
[0029] Calcium Chloride: 5, Macrogol Stearate: 8, Water: 100.
Embodiment 3
[0031] An antistatic finishing agent for wool and its blended fabrics, in parts by weight, consists of the following components:
[0032] Dimethicone: 4, Polymethylhydrogensiloxane: 2,
[0033] Butyl Acrylate: 16, Methyl Nepal: 2, Glycerin: 15,
[0034] Potassium Alkylbenzene Sulfonate: 0.4, Hydroxypropyl Acrylate: 6,
[0035] Calcium Chloride: 4, Macrogol Stearate: 6, Water: 90.
[0036] In the above-mentioned embodiment, the preparation method of described a kind of wool and its blend antistatic finishing agent, comprises the following steps:
[0037] (1) According to the proportion, add butyl acrylate, hydroxypropyl acrylate, polyethylene glycol stearate and glycerin into water, and react for 1 to 3 hours;
[0038] (2) Heat up to 40-60°C, add polydimethylsiloxane and polymethylhydrogensiloxane, and stir for 1-2 hours;
[0039] (3) Cool to room temperature, add the remaining components, stir and mix evenly, and the product can be obtained.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com