Energy-saving wall coating material
A coating material and wall technology, applied in the field of energy-saving wall coating materials, can solve the problems of high additional cost, failure to achieve heat preservation effect, short service life of benzene board materials, etc., and achieve simple production and construction procedures, Good heat preservation and energy saving effect, high bonding strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0008] An energy-saving wall coating material, characterized in that it includes the following parts by weight: 3-9 parts of sepiolite, 2-3 parts of perlite, 1-6 parts of diatomite, 1-2 parts of zinc powder 2-5 parts of lead oxide, 1-2 parts of zirconia, 15-19 parts of silicon dioxide, 2-9 parts of hydrogen peroxide, 2-9 parts of polypropylene, 20-35 parts of polytetrafluoroethylene gum, alcohol 15-20 parts of acid resin, 20-28 parts of melamine resin, 9-16 parts of clam shell powder, 14-18 parts of conch shell powder, 5-9 parts of light plaster, 1-3 parts of perlite, high alumina 10-20 parts of cement.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com