A care agent, anti-wrinkle finishing technology, applied in fiber treatment, textiles and papermaking, etc., can solve the problems of easy wrinkling of fabrics, affect the appearance of fabrics, unsatisfactory antibacterial effect, etc., achieve high antibacterial rate, improve wearing performance, and protect the human body. health effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] The formula of fabric antibacterial anti-wrinkle care agent of the present invention is as follows:
[0015] Polyoxyethylene ether 6kg, dimethyl urea 4kg, sodium polyacrylate 4kg, hydroxyethyl cellulose 2.5kg, sodium alkylbenzene sulfonate 4kg, urea 1.5kg, potassium nitrate 1.5kg, potassium oxalate 0.4kg, sodium alginate 0.25kg, ethanol 4kg, water 55kg.
[0016] The preparation method of fabric antibacterial anti-wrinkle care agent of the present invention is:
[0017] Mix the ingredients in the recipe amount and stir evenly.
[0018] The antibacterial anti-wrinkle finishing method of fabric of the present invention is as follows:
[0019] (1) Immerse the fabric in the antibacterial and anti-wrinkle care agent at room temperature for 10 minutes, wherein the dosage of the antibacterial and anti-wrinkle care agent is 2.0% o.w.f, and the bath ratio is 1:25;
[0020] (2) Dehydration;
[0021] (3) Drying: Dry the fabric at 85°C.
Embodiment 2
[0023] The formula of fabric antibacterial anti-wrinkle care agent of the present invention is as follows:
[0024] Polyoxyethylene ether 8kg, dimethyl urea 3kg, sodium polyacrylate 3kg, hydroxyethyl cellulose 2kg, sodium alkylbenzene sulfonate 5kg, urea 1kg, potassium nitrate 2kg, potassium oxalate 0.3kg, sodium alginate 0.2kg, Ethanol 3kg, water 50kg.
[0025] The preparation method of fabric antibacterial anti-wrinkle care agent of the present invention is:
[0026] Mix the ingredients in the recipe amount and stir evenly.
[0027] The antibacterial anti-wrinkle finishing method of fabric of the present invention is as follows:
[0028] (1) Immerse the fabric in the antibacterial and anti-wrinkle care agent at room temperature for 12 minutes, wherein the dosage of the antibacterial and anti-wrinkle care agent is 3.0% o.w.f, and the liquor ratio is 1:30;
[0029] (2) Dehydration;
[0030] (3) Drying: Dry the fabric at 80°C.
Embodiment 3
[0032] The formula of fabric antibacterial anti-wrinkle care agent of the present invention is as follows:
[0033] Polyoxyethylene ether 5kg, dimethyl urea 5kg, sodium polyacrylate 5kg, hydroxyethyl cellulose 3kg, sodium alkylbenzene sulfonate 3kg, urea 2kg, potassium nitrate 1kg, potassium oxalate 0.5kg, sodium alginate 0.3kg, Ethanol 5kg, water 60kg.
[0034] The preparation method of fabric antibacterial anti-wrinkle care agent of the present invention is:
[0035] Mix the ingredients in the recipe amount and stir evenly.
[0036] The antibacterial anti-wrinkle finishing method of fabric of the present invention is as follows:
[0037] (1) Immerse the fabric in the antibacterial and anti-wrinkle care agent at room temperature for 8 minutes, wherein the dosage of the antibacterial and anti-wrinkle care agent is 1.0% o.w.f, and the bath ratio is 1:20;
[0038] (2) Dehydration;
[0039] (3) Drying: Dry the fabric at 90°C.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com