A technology of sewage treatment agent and adsorbent, which is applied in the field of sewage treatment agent and preparation, can solve the problems of poor sewage treatment effect, etc., and achieve the effect of excellent coagulation effect, good flocculation purification effect and strong adsorption capacity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0020] The preparation method of the sewage treatment agent includes grinding bentonite and adsorbate into powder, mixing and stirring ferric chloride, polyacrylamide, sodium chloride, bentonite, adsorbate, cornstarch and sugar according to the weight ratio .
[0021] The sewage treatment agent has wide sources of raw materials and low cost. The selected ferric chloride is easily soluble in water, has excellent coagulation effect, good product stability, and good flocculation purification effect; the adsorbent can absorb suspended particles in sewage and particles that are not easily soluble in water; since the adsorbate includes sawdust , straw powder, activated carbon, and rice husk, among which activated carbon accounts for one-third of the total weight of the adsorbate, which has a stronger adsorption capacity; adding cornstarch and sugar to the sewage treatment agent can further improve the adsorption and flocculation capacity .
Embodiment 1
[0023] According to the parts by weight of each component, take respectively: 10 parts of ferric chloride, 5 parts of polyacrylamide, 10 parts of sodium chloride, 20 parts of bentonite, 10 parts of adsorbate, 10 parts of cornstarch and 3 parts of sugar.
[0024] Prepare the ingredients according to the weight parts, grind the bentonite and the adsorbate into powder, mix and stir ferric chloride, polyacrylamide, sodium chloride, bentonite, adsorbate, corn starch, and sugar according to the weight ratio .
Embodiment 2
[0026] According to the parts by weight of each component, take respectively: 12 parts of ferric trichloride, 7 parts of polyacrylamide, 12 parts of sodium chloride, 24 parts of bentonite, 12 parts of adsorbate, 12 parts of cornstarch and 4 parts of sugar.
[0027] Prepare the ingredients according to the weight parts, grind the bentonite and the adsorbate into powder, mix and stir ferric chloride, polyacrylamide, sodium chloride, bentonite, adsorbate, corn starch, and sugar according to the weight ratio .
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com