Bacteriostatic agent, preparation method thereof, and water purifying device
The technology of a water purification device and a bacteriostatic agent is applied in the field of bacteriostatic agent and its preparation, and water purification device, which can solve the problems of high silver dissolution rate, need to improve the bacteriostatic rate, expensive equipment, etc., so as to improve the bacteriostatic effect. , Excellent bacteriostatic effect, not easy to secondary pollution effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0019] The invention provides a kind of preparation method of antibacterial agent, comprising:
[0020] The 13×zeolite molecular sieve is placed in the copper ion solution to obtain the copper ion-loaded molecular sieve.
[0021] Molecular sieve is a crystalline aluminosilicate, which has the structure and characteristics of a crystal. The surface is a solid skeleton, and the internal pores can play the role of adsorbing molecules. The pores are connected with each other by channels, and the molecules pass through them. Molecular sieve powder has a strong polarity and Coulomb field inside the crystal pores through the physical adsorption of the van der Waals force of the substance, and shows a strong adsorption capacity for polar molecules and unsaturated molecules. Moreover, the pore size distribution of the molecular sieve is very uniform, and only substances with a molecular diameter smaller than the pore diameter can enter the crystal cavity of the molecular sieve. The p...
Embodiment 1
[0040] Take the molecular sieve with a particle size of 100 mesh to 120 mesh and the molecular sieve with a particle size of 60 mesh to 100 mesh with a weight ratio of 6.5:1, place the above molecular sieve in a copper sulfate solution with a concentration of 0.5mol / L for 3 days, and then centrifuge. The molecular sieve is washed with deionized water until there is no copper ion in the washing liquid, and then dried to obtain the copper-supported molecular sieve.
Embodiment 2
[0042] 13 × zeolite molecular sieve is mixed with NaF and EDTA, dried, the addition of NaF is 1% of the mass of 13 × zeolite molecular sieve; the addition of EDTA is 4% of the mass of 13 × zeolite molecular sieve to obtain the modified 13 × zeolite molecular sieve.
[0043] Take the above-mentioned modified 13×zeolite molecular sieve of 60 mesh to 100 mesh, put it in a copper sulfate solution with a concentration of 0.4mol / L for 2 days, and then centrifuge it, and soak and wash the molecular sieve in a 0.1mol / L sodium silicate aqueous solution until Dry the washing solution without copper ions to obtain the copper-loaded molecular sieve.
PUM
Property | Measurement | Unit |
---|---|---|
particle size (mesh) | aaaaa | aaaaa |
particle size (mesh) | aaaaa | aaaaa |
particle size (mesh) | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
![application no application](https://static-eureka.patsnap.com/ssr/23.2.0/_nuxt/application.06fe782c.png)
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com