Preparation process of traditional Chinese medicine rubber electuary medicine and paste
A preparation process and technology of rubber ointment, applied in the field of biomedicine, can solve the problems of insufficient emulsification and fusion of the matrix, insufficient viscosity of the paste, oil leakage, etc., and achieve the effects of facilitating transdermal absorption, moderate viscosity and long-lasting efficacy.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A preparation process of traditional Chinese medicine rubber ointment paste includes the following steps:
[0022] (1) Rubber cutting: Put the rubber on the working surface under the cutting knife of the rubber cutting machine, and cut it into long strips of 10-15cm for use;
[0023] (2) Rubber mixing: Adjust the roller distance of the rubber mixing machine to 8-10mm, and put the cut long strips of rubber into the feeding position between the two rollers of the rubber mixing machine one after another. The amount of material added each time should not exceed 25kg, and turn on the machine Refine the rubber to form a mesh film with a thickness of 2-3mm for use;
[0024] (3) Foam: Put the mesh film into the container, and then add 120# gasoline to the container. The weight ratio of the 120# gasoline to the mesh film is 3-4:1. After fully stirring, it is sealed and soaked for more than 24 hours , During the airtight soaking process, stir once every 6 hours until the mesh film is c...
Embodiment 2
[0035] A preparation process of traditional Chinese medicine rubber ointment paste includes the following steps:
[0036] (1) Rubber cutting: Put the rubber on the working surface under the cutting knife of the rubber cutting machine, and cut it into long strips of 10-15cm for use;
[0037] (2) Rubber mixing: Adjust the roller distance of the rubber mixing machine to 8-10mm, and put the cut long strips of rubber into the feeding position between the two rollers of the rubber mixing machine one after another. The amount of material added each time should not exceed 25kg, and turn on the machine Refine the rubber to form a mesh film with a thickness of 2-3mm for use;
[0038] (3) Foam: Put the mesh film into the container, and then add 120# gasoline to the container. The weight ratio of the 120# gasoline to the mesh film is 3-4:1. After fully stirring, it is sealed and soaked for more than 24 hours , During the airtight soaking process, stir once every 6 hours until the mesh film is c...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com