Embodiment 1
[0018] Take the following raw materials by weight:
[0019]
[0020] The lubricant is a mixture of polytetrafluoroethylene and sulfated castor oil with a mass ratio of 6:2.
[0021] The cellulose is a mixture of hydroxypropylmethylcellulose, hydroxyethylmethylcellulose and methylcellulose with a mass ratio of 1:3:2.
[0022] The thickener is a mixture of xanthan gum and carrageenan with a mass ratio of 3:2.
[0023] The preparation method of special cleaning and anti-scaling agent for papermaking is as follows:
[0024] Put deionized water into the reaction kettle, raise the temperature to 50°C, add polyaspartic acid and sodium diacetate lubricant, stir evenly, add cellulose while stirring, stir until completely dissolved, then add lubricant in turn , sodium dodecylbenzenesulfonate, sodium gluconate and thickener, stir for 60 minutes, keep warm for 100 minutes, and cool to room temperature.
Embodiment 2
[0026] Take the following raw materials by weight:
[0027]
[0028] The lubricant is a mixture of polytetrafluoroethylene and sulfated castor oil with a mass ratio of 7:3.
[0029] The cellulose is a mixture of hydroxypropylmethylcellulose, hydroxyethylmethylcellulose and methylcellulose with a mass ratio of 2:4:3.
[0030] The thickener is a mixture of xanthan gum and carrageenan with a mass ratio of 4:3.
[0031] The preparation method of special cleaning and anti-scaling agent for papermaking is as follows:
[0032] Put deionized water into the reaction kettle, raise the temperature to 55°C, add polyaspartic acid and sodium diacetate lubricant, stir evenly, add cellulose while stirring, stir until completely dissolved, then add lubricant in turn , sodium dodecylbenzenesulfonate, sodium gluconate and thickener, stir for 50 minutes, keep warm for 90 minutes, and cool to room temperature.
Embodiment 3
[0034] Take the following raw materials by weight:
[0035]
[0036] Described lubricant is the mixture of polytetrafluoroethylene and sulfated castor oil that mass ratio is 8:3;
[0037] Described cellulose is the mixture of hydroxypropyl methylcellulose, hydroxyethyl methylcellulose and methylcellulose with a mass ratio of 3:5:4;
[0038] The thickener is a mixture of xanthan gum and carrageenan with a mass ratio of 5:3.
[0039] The preparation method of special cleaning and anti-scaling agent for papermaking is as follows:
[0040] Put deionized water into the reaction kettle, raise the temperature to 60°C, add polyaspartic acid and sodium diacetate lubricant, stir evenly, add cellulose while stirring, stir until completely dissolved, then add lubricant in turn , sodium dodecylbenzenesulfonate, sodium gluconate and thickener, stir for 45 minutes, keep warm for 80 minutes, and cool to room temperature.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com