Textile auxiliary agent for auxiliary textile sizing and preparation method thereof
A textile auxiliaries and textile technology, applied in the field of textile auxiliaries for assisting textile sizing and its preparation, can solve the problems of little help in sizing effects, insignificant effects, and large dosage required
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0009] The preparation method of the textile auxiliaries of described auxiliary textile sizing comprises the following steps:
[0010] (1) Weigh each raw material according to parts by weight;
[0011] (2) Sodium dioctyl sulfosuccinate, ethyl formamidothiazole acetate, propyltriethoxysilane, 5-aminolevulinic acid, zinc phenolsulfonate, diphenyltridecyl phosphite , laurate, and polymethylsilicone resin, add 10% NaOH solution to adjust the pH to 8.5, and stir at 7500-8500r / m for 6-10h;
[0012] (3) Heat the stirred mixture to 65-75°C, then add azobisisobutyronitrile, nonylphenol polyoxyethylene ether, hydroxypropyl methylcellulose, and nano-graphite powder, and carry out the process in an ultrasonic machine. Ultrasound for the first time, then add cross-linking agent and softener, and perform the second ultrasonic to obtain the finished product.
[0013] Preferably, in the step (3), the first ultrasonic power is 800w, and the ultrasonic time is 6-7h, and the second ultrasonic ...
Embodiment 1
[0019] (1) Weigh 45 parts of dioctyl sodium sulfosuccinate, 40 parts of ethyl formylaminothiazole acetate, 35 parts of propyltriethoxysilane, 35 parts of 5-aminolevulinic acid, sulfonol Zinc acid 30 parts, diphenyltridecyl phosphite 25 parts, laurate 20 parts, polymethyl silicone resin 15 parts, azobisisobutyronitrile 15 parts, nonylphenol polyoxyethylene ether 10 parts, 5 parts of hydroxypropyl methylcellulose, 5 parts of nano graphite powder, 5 parts of polyisocyanate, 5 parts of silicone oil softener;
[0020] (2) Sodium dioctyl sulfosuccinate, ethyl formamidothiazole acetate, propyltriethoxysilane, 5-aminolevulinic acid, zinc phenolsulfonate, diphenyltridecyl phosphite , laurate, and polymethylsilicone resin, add 10% NaOH solution to adjust the pH to 8.5, and stir for 6 hours at 7500r / m;
[0021] (3) Heat the stirred mixture to 65°C, then add azobisisobutyronitrile, nonylphenol polyoxyethylene ether, hydroxypropyl methylcellulose, and nano-graphite powder, and perform the...
Embodiment 2
[0024] (1) Weigh 50 parts of dioctyl sodium sulfosuccinate, 45 parts of ethyl formylaminothiazole acetate, 40 parts of propyltriethoxysilane, 40 parts of 5-aminolevulinic acid, sulfonol Zinc acid 35 parts, diphenyltridecyl phosphite 30 parts, laurate 25 parts, polymethyl silicone resin 20 parts, azobisisobutyronitrile 20 parts, nonylphenol polyoxyethylene ether 15 parts, 10 parts of hydroxypropyl methylcellulose, 7 parts of nano graphite powder, 7 parts of polyether amino-modified polysiloxane, 7 parts of ester quaternary ammonium salt;
[0025] (2) Sodium dioctyl sulfosuccinate, ethyl formamidothiazole acetate, propyltriethoxysilane, 5-aminolevulinic acid, zinc phenolsulfonate, diphenyltridecyl phosphite , laurate, polymethyl silicone resin mixed, adding 10% NaOH solution to adjust the pH to 8.5, stirring at 8000r / m for 8h;
[0026] (3) Heat the stirred mixture to 70°C, then add azobisisobutyronitrile, nonylphenol polyoxyethylene ether, hydroxypropyl methylcellulose, and nan...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com