Pressure sore prevention gasket
A technology for preventing pressure ulcers and gaskets, applied in medical science, surgery, etc., can solve the problems of insufficient blood supply to local tissues, debris in the folds of bed sheets, malnutrition in the whole body, etc. The effect of the pressure ulcer effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0104] An anti-pressure sore gasket, the composition and parts by weight are as follows:
[0105]
[0106] The specific preparation is as follows:
[0107] (1) Weigh each raw material according to the above ratio, and then put it in a mixer, mix it at 60-90°C for 30-50 minutes, and let the ratio raw materials mix with each other evenly;
[0108] ⑵Put the material mixed evenly in step ⑴ into the granulator for calendering. The temperature of the molding machine is controlled as follows: first stage: 130-150°C, second stage: 170-200°C, third and fourth stage: 220-240°C , Five and six stages: 210-230°C, each stage is 1-10min, and the thermoplastic composition is obtained after the rolling is completed.
[0109] ⑶ Pass the thermoplastic composition through calendering equipment and injection molding equipment to complete the required shape and size of the product.
Embodiment 2
[0111] An anti-pressure sore gasket, the composition and parts by weight are as follows:
[0112]
[0113] Key product characteristics of the anti-pressure sore gasket provided by the present invention (both embodiment 1 and embodiment 2 meet the requirements)
[0114] ⑴Hardness range: Shore A 0-95.
[0115] ⑵Using temperature performance: It can be processed at high temperature. It has good temperature resistance, its embrittlement temperature ≤ -60°C, the highest operating temperature reaches 149°C, and its decomposition temperature is greater than 270°C in an oxygen atmosphere.
[0116] ⑶ Aging resistance performance: the decline rate of performance is less than 10% after aging in an artificial accelerated aging box for one week, and the performance decline rate is less than 10% after 100 hours of ozone aging (38°C).
[0117] ⑷Environmentally friendly performance: Thermoplastic polymers can be used without vulcanization, which meets environmental protection requirements...
PUM
| Property | Measurement | Unit |
|---|---|---|
| brittleness temperature | aaaaa | aaaaa |
| service temperature | aaaaa | aaaaa |
| decomposition temperature | aaaaa | aaaaa |