[0017] This antibacterial antique brick contains the following raw materials in parts by weight: 500 parts of fly ash, 400 parts of clay, 310 parts of cement, 300 parts of quartz sand, 300 parts of slag, 30 parts of nano zinc oxide, 15 parts of epoxy resin, hexadecane 10 parts of trimethylammonium bromide, appropriate amount of water.
[0018] The production method is as follows:
[0019] A. Crush and grind fly ash, clay, quartz sand, slag, and epoxy resin to 150-200 mesh for later use;
[0020] B, add cement, nano-zinc oxide, cetyltrimethylammonium bromide to the powder obtained in step A and stir evenly, set aside;
[0021] C. Add an appropriate amount of water to the obtained step B, stir evenly, make the water content reach 15%, inject it into the mold and press it into adobe;
[0022] D. Carry out thermal insulation heat treatment to the adobe obtained in step C, the heating temperature is 1200°C, the heating time is 0.75h, and the temperature can be cooled.
Embodiment 2
[0024] This antibacterial antique brick contains the following raw materials in parts by weight: 600 parts of fly ash, 450 parts of clay, 320 parts of cement, 320 parts of corundum, 320 parts of steel slag, 50 parts of nano-zinc oxide, 20 parts of rubber, cetyl trimethyl 15 parts of ammonium bromide, appropriate amount of water.
[0025] The production method is as follows:
[0026] A. Crush and grind fly ash, clay, corundum, steel slag, and rubber to 150-200 mesh, and set aside;
[0027] B, add cement, nano-zinc oxide, cetyltrimethylammonium bromide to the powder obtained in step A and stir evenly, set aside;
[0028] C. Add an appropriate amount of water to the obtained step B, stir evenly, and make the water content reach 20%, inject it into a mold and press it into adobe;
[0029] D. Carry out thermal insulation heat treatment to the adobe obtained in step C, the heating temperature is 200°C, the heating time is 1.5h, and the temperature can be obtained by cooling.