Embodiment 1
[0014] Embodiment 1, the inorganic type engine coolant of the present invention comprises the following components in parts by weight: 43 parts of ethylene glycol, 0.12 part of phosphoric acid, 0.6 part of borax, 0.1 part of urotropine, 0.1 part of sodium silicate, benzotriazine 0.05 parts of azole, 0.5 parts of defoamer, and 55.53 parts of base liquid.
[0015] The preparation method of the inorganic type engine coolant comprises the following steps: first, take 20 parts of deionized water and put it into the reaction kettle, adjust the temperature so that the temperature in the reaction kettle is controlled at 40-50°C, turn on the electric stirring, and the rotation speed is 30-50r / h min; then add 0.6 parts of borax, 0.1 parts of sodium silicate, and 0.1 part of urotropine to the reaction kettle in sequence, and stir for 20 to 40 minutes until completely dissolved; then add 43 parts of ethylene glycol into the reaction kettle, Stir for 10 to 20 minutes until uniformly mixed;...
Embodiment 2
[0019] Embodiment 2, the inorganic type engine coolant of the present invention comprises the following components in parts by weight: 42 parts of ethylene glycol, 0.13 parts of phosphoric acid, 0.5 part of borax, 0.2 part of urotropine, 0.05 part of sodium silicate, benzotriazepam 0.1 part of azole, 0.6 part of defoamer, 56.42 parts of base liquid.
[0020] The preparation method is basically the same as in Example 1.
Embodiment 3
[0021] Embodiment 3, the inorganic type engine coolant of the present invention comprises the following components in parts by weight: 44 parts of ethylene glycol, 0.11 part of phosphoric acid, 0.7 part of borax, 0.15 part of urotropine, 0.15 part of sodium silicate, benzotriazepam 0.1 part of azole, 0.8 part of defoamer, 53.99 parts of base liquid.
[0022] The preparation method is basically the same as in Example 1.
[0023] Main physical and chemical index of the present invention is:
[0024]
[0025]
[0026] The main use performance index of the present invention is:
[0027]
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 