A kind of preparation method of stable working cable
A stable, cable technology, applied in cable/conductor manufacturing, conductor/cable insulation, circuits, etc., can solve the problems of buried cable corrosion, shorten cable life, increase in harmful substances, etc., and achieve heat resistance, corrosion resistance and structural strength. Improve, improve material properties, good physical properties
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0036] The preparation method of the stable working cable of the present embodiment comprises the following steps:
[0037] (1) Ingredients: The mass percentage of each component in the raw material is: C: 0.05%, Fe: 1.25%, Mn: 0.42%, S: ≤0.020%, P: ≤0.030%, Cr: 0.13%, Ni: 1.35%, Zn : 1.75%, Cu: 7.95%, Mo: 0.03%, Ti: 1.47%, Pd: 0.02%, Pt: 0.21%, Au: 0.41%, W: 0.05%, Nd: 0.03%, Ce: 0.03%, Eu : 0.01%, Lu: 0.02%, the balance is Ag;
[0038] (2) Smelting: heating and melting the cable raw materials with stable work, as follows:
[0039] a. Add the raw materials into the furnace according to the mass percentage of each component in the predetermined working stable cable, raise the temperature in the furnace to 1650 degrees Celsius to 1680 degrees Celsius, and the raw materials are smelted to form an alloy solution;
[0040] b. Cool the alloy solution obtained in the previous step, and use water cooling to cool the alloy solution to room temperature at a cooling rate of 26-28°C / s;...
Embodiment 2
[0057] The preparation method of the stable working cable of the present embodiment comprises the following steps:
[0058] (1) Ingredients: The mass percentage of each component in the raw material is: C: 0.15%, Fe: 1.56%, Mn: 0.73%, S: ≤0.020%, P: ≤0.030%, Cr: 0.26%, Ni: 1.63%, Zn : 1.96%, Cu: 8.46%, Mo: 0.06%, Ti: 1.69%, Pd: 0.05%, Pt: 0.33%, Au: 0.62%, W: 0.15%, Nd: 0.06%, Ce: 0.07%, Eu : 0.04%, Lu: 0.03%, the balance is Ag;
[0059] (2) Smelting: heating and melting the cable raw materials with stable work, as follows:
[0060] a. Add the raw materials into the furnace according to the mass percentage of each component in the predetermined working stable cable, raise the temperature in the furnace to 1650 degrees Celsius to 1680 degrees Celsius, and the raw materials are smelted to form an alloy solution;
[0061] b. Cool the alloy solution obtained in the previous step, and use water cooling to cool the alloy solution to room temperature at a cooling rate of 26-28°C / s;...