Hybrid slag metallurgy smelting reduction recycling method
A recovery method and slag technology, applied in the recovery field of mixed slag metallurgical smelting reduction, can solve the problems of high metal recovery rate, short reaction time, and low production cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0134] A recovery method for metallurgical smelting reduction of mixed slag is carried out according to the following steps:
[0135] Step 1, mixed slag metallurgical smelting reduction
[0136] The molten blast furnace slag obtained from the slag outlet and heated to molten electric furnace steelmaking steel slag, according to the mass ratio, molten blast furnace slag: electric furnace steelmaking steel slag = (200:300) kg batching, adding preheating temperature is 1200 ° C In the thermal insulation pit, the reaction mixed slag is formed by mixing. During the slag mixing process, the iron oxide in the slag undergoes a melting reduction reaction. The reaction mixed slag is monitored in real time, and the following (a), (b) and ( c) Three parameters:
[0137] (a) The temperature of the reaction mixed slag is 1300-1580°C; (b) The reaction mixed slag is fully mixed; (c) In the reaction mixed slag, the mass concentration of FeO is ≤ 1.0%; the control method is as follows:
[0138]...
Embodiment 2
[0150] A recovery method for metallurgical smelting reduction of mixed slag is carried out according to the following steps:
[0151] Step 1, mixed slag metallurgical smelting reduction
[0152] The molten blast furnace slag obtained from the slag outlet and the molten converter steelmaking steel slag obtained from the slag outlet are, by mass ratio, molten blast furnace slag: converter steelmaking steel slag=(50:300) kg batching, add Converter, mixed to form reaction mixed slag, real-time monitoring of reaction mixed slag, through regulation and control to ensure the following three parameters (a), (b) and (c) at the same time:
[0153] (a) The temperature of the reaction mixed slag is 1350-1650° C.; (b) The reaction mixed slag is fully mixed; (c) In the reaction mixed slag, the mass concentration of FeO is ≤ 1.0%. The control method is as follows:
[0154] Corresponding to (a): The temperature of the reaction mixed slag is 1655°C, which exceeds the set temperature range, an...
Embodiment 3
[0166] A recovery method for metallurgical smelting reduction of mixed slag is carried out according to the following steps:
[0167] Step 1, mixed slag metallurgical smelting reduction
[0168] The molten blast furnace slag obtained from the slag outlet and the converter steelmaking steel slag heated to the molten state, according to the mass ratio, molten blast furnace slag: converter steelmaking steel slag=(20:400) kg batching, add in the blast furnace, mix The reaction mixed slag is formed, the reaction mixed slag is monitored in real time, and the following three parameters (a), (b) and (c) are guaranteed at the same time through regulation and control:
[0169] (a) The temperature of the reaction mixed slag is 1350-1650° C.; (b) The reaction mixed slag is fully mixed; (c) In the reaction mixed slag, the mass concentration of FeO is ≤ 1.0%. The control method is as follows:
[0170] Corresponding to (a): The temperature of the reaction mixed slag is 1660°C. If it exceeds...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com