Black liquid dispersing dye with characteristics of high color fastness and low brightness, and preparation method thereof
A liquid disperse dye, high color fastness technology, applied in the field of textile printing and dyeing, to achieve the effect of less waste water treatment, improved soaping color fastness and wet rubbing fastness, and less dye floating color
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0052] 1) Add 8.0g of acrylic acid, 4.0g of acrylonitrile, 2.0g of ethyl acrylate, 16.0g of vinylpyridine, an appropriate amount of emulsifier (1.0g of fatty alcohol (C12-18) polyoxyethylene ether (15) sodium sulfonate, 0.5g Emulsifier SP-80) mixed with 68.5g of water, and fully stirred into emulsion A;
[0053] 2) Take 1 / 3 of the mass of emulsion A, add 0.9g of ammonium persulfate, slowly raise the temperature to 80°C, react at this temperature for 10 minutes, then slowly add the remaining 2 / 3 of emulsion A within 60 minutes, drop After the addition is completed, react at a constant temperature of 85°C for 1 hour to obtain prepolymer A;
[0054] 3) Add an appropriate amount of hydrogen peroxide and ferrous sulfate to the above prepolymer at a constant temperature of 85°C, and continue the reaction for 2 hours to obtain polyacrylic acid copolymer A.
Embodiment 2
[0056] 1) Mix 6.0g of acrylic acid, 5.0g of acrylonitrile, 3.0g of ethyl acrylate, 19.0g of vinylpyridine, an appropriate amount of emulsifier (1.0g of sodium dodecylsulfonate, 0.5g of emulsifier SP-80) and 65.5 g of water Mix and stir well into Emulsion B;
[0057] 2) Take 1 / 3 of the mass of emulsion A, add 1.0g of ammonium persulfate, slowly raise the temperature to 80°C, react at this temperature for 1 min, then slowly add the remaining 2 / 3 of emulsion A within 60 min, drop After the addition is completed, react at a constant temperature of 85°C for 1 hour to obtain prepolymer B;
[0058] 3) Add an appropriate amount of hydrogen peroxide and ferrous sulfate to the above prepolymer at a constant temperature of 85°C, and continue the reaction for 2 hours to obtain polyacrylic acid copolymer B.
Embodiment 3
[0060] With the red dye of 0.77g structural formula A1, the orange dye of 11.46g structural formula A2, the blue dye of 6.18g structural formula A3, the blue dye of 6.65g structural formula A4, the formaldehyde condensate of 2.0g sodium methyl naphthalenesulfonate, 0.5g Aliphatic amine polyoxyethylene ether (EO=15), 5.0g of polyacrylic acid copolymer A, 0.5g of amino silicone oil, 0.02g of benzisothiazolinone and 66.92g of water were mixed and ground on a zirconia sand mill for 2.5 hours, Prepared liquid disperse dye AA-1.
PUM
![No PUM](https://static-eureka.patsnap.com/ssr/23.2.0/_nuxt/noPUMSmall.5c5f49c7.png)
Abstract
Description
Claims
Application Information
![application no application](https://static-eureka.patsnap.com/ssr/23.2.0/_nuxt/application.06fe782c.png)
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com