Water-based environment-friendly modified kieselguhr oil paint and preparation method thereof
A technology of environmental protection paint and diatomite, applied in the direction of coating, etc., can solve the problems of human body secondary pollution, formaldehyde escape, permanent adsorption, etc., and achieve the effect of protecting the environment, avoiding waste of resources, and easy operation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] A modified diatomite water-based environmental protection paint is characterized in that it comprises the following components by weight: 13 parts of acrylate emulsion; 7 parts of water-based polyurethane synthetic resin; 1.5 parts of dipropylene glycol butyl ether; 17 parts of deionized water; 0.35 parts of polyethylene glycol esters; 9 parts of polyacrylates; 0.2 parts of polyoxypropylene glyceryl ether; 0.5 parts of dioctyl sodium sulfosuccinate; 0.15 parts of zinc oxide; 11 parts of white pulp; 25 parts of modified diatomaceous earth; 0.6 parts of water-based silane coupling agent.
[0027] Modified diatomite adopts the following preparation method:
[0028] 1) Weigh 500 g of diatomite raw soil and put it into a 2L beaker, slowly add 500 mL of 4 mol. L -1 Hydrochloric acid solution, after the dropwise addition, put it into a water bath at 80°C and soak for 2 hours, filter and wash with suction; then add 500mL4mol. L -1 Potassium hydroxide solution, soaked for 5 ...
Embodiment 2
[0038]A modified diatomite water-based environmental protection paint is characterized in that it comprises the following components by weight: 10 parts of acrylate emulsion; 6 parts of water-based polyurethane synthetic resin; 1 part of dipropylene glycol butyl ether; 16 parts of deionized water; fatty acid 0.2 part of polyethylene glycol ester; 8 parts of associative polyurethane; 0.1 part of polyoxyethylene polyoxypropylene glyceryl ether; 0.3 part of diisooctyl sodium sulfosuccinate; 0.1 part of zinc oxide; 0.1 part of alkane; 7 parts of titanium white paste; 20 parts of modified diatomaceous earth; 0.5 part of water-based silane coupling agent.
[0039] Modified diatomite adopts the following preparation method:
[0040] 1) Weigh 500 g of diatomite raw soil and put it into a 2L beaker, slowly add 500 mL of 4 mol. L -1 Hydrochloric acid solution, after the dropwise addition, put it into a water bath at 80°C and soak for 2 hours, filter and wash with suction; then add 500...
PUM
Property | Measurement | Unit |
---|---|---|
specific surface area | aaaaa | aaaaa |
porosity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com