[0007] Example 1
[0008] Mix 16 parts of ethylene glycol, 6 parts of 2-hydroxyethyl methacrylate, 6 parts of methyl methacrylate, 4 parts of lauryl methacrylate, 2 parts of magnesium chloride, 2 parts of glycerin rosin resin, and 10 parts of ethyl acetate. , 10 parts of butyl acetate, 20 parts of sodium carbonate, 20 parts of polyisobutyl ester, 10 parts of phosphoric acid triesters, 20 parts of lauryl methacrylate, 20 parts of zinc nitrate hexahydrate, 10 parts of benzoyl peroxide, poly 2 20 parts of ethylene acetylene, 10 parts of naphthenic acid, 400 parts of deionized water are put into the reactor, and the mixture is continuously stirred, and the mixture is heated to 60° C., and the product is obtained after uniform stirring.
Example Embodiment
[0009] Example 2
[0010] Combine 24 parts of ethylene glycol, 9 parts of 2-hydroxyethyl methacrylate, 7 parts of methyl methacrylate, 5 parts of lauryl methacrylate, 4 parts of magnesium chloride, 3 parts of glycerin rosin resin, and 15 parts of ethyl acetate , 20 parts of butyl acetate, 40 parts of sodium carbonate, 25 parts of polyisobutyl ester, 15 parts of phosphoric acid triester, 25 parts of lauryl methacrylate, 25 parts of zinc nitrate hexahydrate, 15 parts of benzoyl peroxide, poly-two 25 parts of ethylene acetylene, 13 parts of naphthenic acid, and 500 parts of deionized water are put into the reactor, continuously stirred, heated to 60°C after the mixing is complete, and the product is obtained after uniform stirring.
Example Embodiment
[0011] Example 3
[0012] Mix 32 parts of ethylene glycol, 12 parts of 2-hydroxyethyl methacrylate, 8 parts of methyl methacrylate, 6 parts of lauryl methacrylate, 6 parts of magnesium chloride, 4 parts of glycerin rosin resin, and 20 parts of ethyl acetate. , 30 parts of butyl acetate, 60 parts of sodium carbonate, 30 parts of polyisobutyl ester, 20 parts of phosphoric acid triesters, 30 parts of lauryl methacrylate, 30 parts of zinc nitrate hexahydrate, 20 parts of benzoyl peroxide, poly 2 30 parts of ethylene acetylene, 16 parts of naphthenic acid, and 600 parts of deionized water are put into the reactor, continuously stirred, heated to 60°C after the mixing is completed, and the product is obtained after uniform stirring.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap