Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

Production method of PP (polypropylene) thin film

A technology of polypropylene film and production method, which is applied in the production of polypropylene film and the field of polymer materials, can solve the problems of insufficient density, unreasonable process conditions, uneven products, etc.

Pending Publication Date: 2018-01-19
镇江春环密封件集团有限公司
View PDF2 Cites 1 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0002] Plastic film is a kind of film with a wide range of applications, and with the development of society, there are more and more demands for plastic films in all walks of life. Plastic films are mainly used for packaging and laminating, and have been widely used in food , medicine, chemical industry and other fields have brought great convenience to people's life, and polypropylene has good heat resistance and light weight performance, and its market share is also high, so it promotes the development of polypropylene film technology Development, especially the polypropylene film made has the advantages of good heat resistance, acid and alkali resistance, friction resistance, light weight, non-toxic, odorless and so on, which makes it develop very rapidly. However, the existing polypropylene film has Therefore, its tear resistance, oxidation resistance, corrosion resistance and smoothness cannot be guaranteed, especially the unreasonable process conditions in the production process, which makes the product have defects such as unevenness and insufficient density

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0014] The production method of the polypropylene film of the present embodiment, comprises the following steps:

[0015] A. Weigh 50 parts of random copolymer polypropylene, 15 parts of block copolymer polypropylene, 8 parts of polyethylene, 7 parts of calcium carbonate, 1 part of silicon dioxide, 6 parts of amino resin, and 13 parts of stearyl alcohol by weight. into the reactor;

[0016] B. Introduce nitrogen gas into the reactor and heat for 20 minutes, the heating temperature is 150°C, then weigh 2 parts of glass fiber, 3 parts of talcum powder, and 1 part of carbon black by weight and put them into the reactor to continue heating and reacting for 40 minutes minutes, the heating temperature is 200°C;

[0017] C. Feed the reacted compound into the twin-screw extruder through the constant temperature hopper for processing, wherein the temperature of the constant temperature hopper is controlled at 80°C;

[0018] D. The twin-screw extruded strips of the twin-screw extruder...

Embodiment 2

[0020] The production method of the polypropylene film of the present embodiment, comprises the following steps:

[0021] A. Weigh 55 parts of random copolymer polypropylene, 17 parts of block copolymer polypropylene, 9 parts of polyethylene, 8 parts of calcium carbonate, 1 part of silicon dioxide, 7 parts of amino resin, and 14 parts of stearyl alcohol by weight. into the reactor;

[0022] B. Feed nitrogen into the reactor and heat for 25 minutes. The heating temperature is 165°C. Then weigh 2 parts of glass fiber, 4 parts of talcum powder and 2 parts of carbon black by weight and put them into the reactor to continue heating and reacting for 50 minutes. minutes, the heating temperature is 200-230°C;

[0023] C. Feed the reacted compound into the twin-screw extruder through the constant temperature hopper for processing, wherein the temperature of the constant temperature hopper is controlled at 85°C;

[0024] D. The twin-screw extruded strips of the twin-screw extruder are...

Embodiment 3

[0026] The production method of the polypropylene film of the present embodiment, comprises the following steps:

[0027] A. Weigh 60 parts of random copolymer polypropylene, 20 parts of block copolymer polypropylene, 10 parts of polyethylene, 10 parts of calcium carbonate, 2 parts of silicon dioxide, 8 parts of amino resin, and 15 parts of stearyl alcohol by weight. into the reactor;

[0028] B. Feed nitrogen into the reactor and heat for 30 minutes, the heating temperature is 180°C, then weigh 3 parts of glass fiber, 5 parts of talcum powder, and 2 parts of carbon black by weight and put them into the reactor to continue heating and reaction for 60 minutes, the heating temperature is 230°C;

[0029] C. Feed the reacted compound into the twin-screw extruder through the constant temperature hopper for processing, wherein the temperature of the constant temperature hopper is controlled at 90°C;

[0030] D. The twin-screw extruded strips of the twin-screw extruder are air-cool...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a production method of a PP (polypropylene) thin film. The production method comprises steps as follows: A, PP random copolymers, PP block copolymers, polyethylene, calcium carbonate, silicon dioxide, amino resin and octadecanol are weighed and put into a reaction kettle; B, nitrogen is introduced into the reaction kettle, the reaction kettle is heated, then glass fibers, talcum powder and carbon black are weighed and added to the reaction kettle, and the reaction kettle is heated continuously; C, a mixed material obtained after the reaction is sent into a twin-screw extruder through a constant-temperature hopper for processing; D, twin-screw extruded sample strips are air-cooled, then heated in a temperature control chamber and water-cooled, master batch is obtained after air drying and grain-sized dicing, finally, the master batch is put in a plastic film blowing machine and subjected to extruded film blowing, and a finished product is obtained. With the adoption of the method, density and flatness of the product are guaranteed, defects are prevented, the product has the advantages of being good in resistance to heat, acid and base, resistant to wear, light, non-toxic, odor-free and the like, and tear resistance, oxidation resistance, corrosion resistance and smoothness of the product are improved dramatically.

Description

technical field [0001] The invention relates to a polymer material, in particular to a production method of a polypropylene film, which belongs to the technical field of chemical materials. Background technique [0002] Plastic film is a kind of film with a wide range of applications, and with the development of society, there are more and more demands for plastic films in all walks of life. Plastic films are mainly used for packaging and laminating, and have been widely used in food , medicine, chemical industry and other fields have brought great convenience to people's life, and polypropylene has good heat resistance and light weight performance, and its market share is also high, so it promotes the development of polypropylene film technology Development, especially the polypropylene film made has the advantages of good heat resistance, acid and alkali resistance, friction resistance, light weight, non-toxic, odorless and so on, which makes it develop very rapidly. Howev...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C08L23/14C08L53/00C08L23/06C08L61/20C08J5/18
Inventor 刘小芳
Owner 镇江春环密封件集团有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products