A paint and coating technology, which is applied in the direction of architecture and building structure, can solve the problems of not being environmentally friendly, not resistant to acid and alkali, and not easy to clean, and achieve the effect of not being volatile and not producing mold deterioration
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] This embodiment provides a combined coating, which includes component A and component B separately packaged and mixed for use. The component A is the main agent of the coating, and the component B is the film-forming accelerator. The A component and the B component of the coating are firstly mixed thoroughly and then coated on the wall surface, and after a series of reactions, they are naturally cured to form a coating film to protect the wall surface.
[0027] In this embodiment, calculated by weight percentage, the main agent A component includes the following components: nano silica 55%; modified silicone resin 15%; silicone leveling agent 0.4%; alcohol solvent 29.6%. Nano-silica uses sol-gel to synthesize nano-silica, which is the main component of the formed inorganic coating film. During spraying, it can produce a highly stable coating film through sol-gel reaction and hydrolysis and solidification, which is not easy to volatilize and difficult. Reacts with other sub...
Embodiment 2
[0044] This embodiment provides a combined coating including component A and component B used in combination. Calculated by weight percentage, component A of the main agent includes the following components: nano-silica 48%; modified silicone resin 10% ; Organic silicon leveling agent 0.2%; alcohol solvent 41.8%.
[0045] The above-mentioned nano-silica is a sol-gel synthesized nano-silica, which is the main component of the inorganic coating formed on the wall surface. During spraying, it can produce a highly stable coating through sol-gel reaction and hydrolysis curing. It is not easy to volatile and does not react easily with other substances. Among them, the alcohol solvent is preferably isopropanol or butanol or a mixture of the two. The above-mentioned silicone leveling agent adopts the component materials in common coatings, such as polydimethylsiloxane, polyether polyester modified silicone oxide Alkyl, alkyl modified organosiloxane, etc. The composition of component B ...
Embodiment 3
[0047] This embodiment provides a combined coating including component A and component B used in combination. Calculated by weight percentage, component A of the main agent includes the following components: nano silica 60%; modified silicone resin 16% ; Organic silicon leveling agent 0.5%; Alcohol solvent 23.5%.
[0048] The composition of component B in this embodiment is the same as that in the first embodiment above, and the proportion of alcohol solvent can be appropriately increased within its range. At the same time, the coating method of the combination paint provided in the third embodiment is the same as that of the first embodiment, and will not be repeated here.
PUM
Property | Measurement | Unit |
---|---|---|
Thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com