Environment-friendly ecological diatom mud paint and preparation method thereof
A diatom mud coating and ecological technology, applied in the field of architectural coatings, can solve the problems of difficult construction, easy falling off, low bonding strength, etc., and achieve the effects of low cost, high bonding strength, and convenient preparation and use.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0036] In the present embodiment, the environmental protection ecological diatom mud coating comprises the following components in terms of weight percentage: 14% kaolin, 2% wood fiber, 8% magnesium aluminum silicate, 0.3% antifungal agent, 5% rubber powder, light calcium carbonate 15%, calcium hydroxide 8%, diatomite filter aid 12%, titanium dioxide 6%, attapulgite powder 7%, sepiolite powder 3%, and the balance is diatomite.
[0037] Its preparation method comprises the following steps:
[0038] (1) Add kaolin, light calcium carbonate, calcium hydroxide, attapulgite powder, sepiolite powder, wood fiber and rubber powder in the dispersion container, stir evenly, the stirring speed is 330 rpm, and the stirring time is 16min to obtain the premixture;
[0039] (2) Add antifungal agent, magnesium aluminum silicate, titanium dioxide, diatomaceous earth and diatomite filter aid to the pre-mixture in sequence, after adding one component and stir evenly, add another one at a stirring...
Embodiment 2
[0041] In the present embodiment, the environmental protection ecological diatom mud coating comprises the following components in terms of weight percentage: 16% of kaolin, 3% of wood fiber, 7% of magnesium aluminum silicate, 0.2% of mold inhibitor, 4% of rubber powder, light calcium carbonate 16%, calcium hydroxide 10%, diatomite filter aid 10%, titanium dioxide 8%, attapulgite powder 8%, sepiolite powder 4%, and the balance is diatomite.
[0042] Its preparation method comprises the following steps:
[0043] (1) Add kaolin, light calcium carbonate, calcium hydroxide, attapulgite, sepiolite powder, wood fiber and rubber powder into the dispersion container, stir evenly, the stirring rate is 300 rpm, and the stirring time is 30min to obtain the premixture;
[0044](2) Add antifungal agent, magnesium aluminum silicate, titanium dioxide, diatomaceous earth and diatomite filter aid to the pre-mixture in sequence, after adding one component and stir evenly, add another one at a s...
Embodiment 3
[0046] In the present embodiment, the environmental protection ecological diatom mud coating comprises the following components in terms of weight percentage: 13% of kaolin, 2% of wood fiber, 10% of magnesium aluminum silicate, 0.4% of mold inhibitor, 6% of rubber powder, light calcium carbonate 18%, calcium hydroxide 6%, titanium dioxide 8%, attapulgite powder 10%, sepiolite powder 6%, and the balance is diatomaceous earth.
[0047] Its preparation method comprises the following steps:
[0048] (1) Add kaolin, light calcium carbonate, calcium hydroxide, attapulgite powder, sepiolite powder, wood fiber and rubber powder into the dispersion container, stir evenly, the stirring rate is 340 rpm, and the stirring time is 15min to obtain the premixture;
[0049] (2) Add antifungal agent, magnesium aluminum silicate, titanium dioxide and diatomaceous earth to the pre-mixture in turn, and after adding one component, stir evenly before adding another one, the stirring speed is 380 rpm...
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com