A technology of diammonium phosphate and monoammonium phosphate, which is applied in the direction of separation methods, precipitation separation, chemical instruments and methods, etc., can solve the problems of increasing production, easy degradation of polyacrylamide, poor flocculation effect, etc., and achieves reduction of loss and sedimentation The effect of speed acceleration and good solubility
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] Special flocculants for monoammonium phosphate and diammonium phosphate filtration,
[0024] Raw material preparation
[0025] Acrylamide 90-120kg, deionized water 45-60kg, urea 0.5-3kg, thiourea 1-4kg, 2,2 azobis(acetamidopropyl) dihydrochloride 0.001-0.009kg, ethylenediamine Sodium tetraacetate 0.001-0.008kg, ammonium persulfate 0.001-0.008kg, sodium bisulfite 0.001-0.009kg;
[0026] Raw material pretreatment
[0027] After preparing the raw materials, add them to the polymerization tank, inject high-purity nitrogen gas, and turn on the ultraviolet light to initiate polymerization. After 0.5-2 hours, it becomes a translucent rubber block;
[0028] Add the following additives after the raw materials are in the form of rubber blocks
[0029] Put the rubber block into the kneader, add 4-8kg sodium carbonate or 2-8kg sodium hydroxide, 1-8kg urea, pass steam, control the temperature at about 90-110°C, hydrolyze for 2-7 hours, and carry out granulation. Finally, it is d...
Embodiment 2
[0042] Special flocculants for monoammonium phosphate and diammonium phosphate filtration,
[0043] Raw material preparation
[0044] Acrylamide 90-120kg, deionized water 45-60kg, urea 0.5-3kg, thiourea 1-4kg, 2,2 azobis(acetamidopropyl) dihydrochloride 0.001-0.009kg, ethylenediamine Sodium tetraacetate 0.001-0.008kg, ammonium persulfate 0.001-0.008kg, sodium bisulfite 0.001-0.009kg;
[0045] Raw material pretreatment
[0046] After preparing the raw materials, add them to the polymerization tank, inject high-purity nitrogen gas, and turn on the ultraviolet light to initiate polymerization. After 0.5-2 hours, it becomes a translucent rubber block;
[0047] Add the following additives after the raw materials are in the form of rubber blocks
[0048] Put the rubber block into the kneader, add 4-8kg sodium carbonate or 2-8kg sodium hydroxide, 1-8kg urea, pass steam, control the temperature at about 90-110°C, hydrolyze for 2-7 hours, and carry out granulation. Finally, it is d...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com