A glass bottle, imitating porcelain technology, applied in glass manufacturing equipment, glass furnace equipment, manufacturing tools and other directions, can solve the problems of poor chemical stability of glass bottles, fragile and easy to explode, single sensory vision, etc., to improve glass melting rate, Low cost and low energy consumption
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0055] The main ingredients are proportioned according to the following mass fractions: ordinary quartz sand powder 53.89%, lepidolite powder 7.67%, soda ash 18.40%, calcite powder 12.60%, dolomite powder 4.30%;
[0056]The auxiliary materials are proportioned according to the following mass fractions: 0.20% of barite powder, 1.60% of sodium fluorosilicate, 0.60% of sodium sulfate, 0.40% of cobalt oxide, and 0.40% of copper oxide.
[0057] According to the raw materials of the above-mentioned mass fraction ratio, the raw materials of the following parts by weight are weighed successively:
[0058] Main ingredients: ordinary quartz sand powder: 274.2kg, lepidolite powder: 39kg, soda ash 93.6kg, calcite powder 64.1kg, dolomite powder 21.9kg;
[0059] Accessory materials: 1kg of barite powder, 8kg of sodium fluorosilicate, 3kg of sodium sulfate, 2kg of cobalt oxide, and 2kg of copper oxide.
[0060] According to the formula raw material of above-mentioned parts by weight, carry ...
Embodiment 2
[0068] The main ingredients are proportioned according to the following mass fractions: ordinary quartz sand powder 49.5%, lepidolite powder 11.8%, soda ash 18.44%, calcite powder 9.83%, dolomite powder 7.42%;
[0069] The auxiliary materials are proportioned according to the following mass fractions: 1.62% of sodium fluorosilicate, 1.26% of sodium sulfate, and 0.13% of cobalt oxide.
[0070] According to the raw materials of the above-mentioned mass fraction ratio, the raw materials of the following parts by weight are weighed successively:
[0071] 549 kg of plain white quartz sand, 130.9 kg of lithium feldspar, 204.5 kg of soda ash, 109 kg of calcite, 82.3 kg of dolomite, 18 kg of sodium fluorosilicate, 14 kg of sodium sulfate, and 1.4 kg of cobalt oxide.
[0072] According to the formula raw material of above-mentioned parts by weight, carry out the preparation method of the formula of cobalt blue imitation porcelain glass bottle, comprise the following steps:
[0073] Th...
PUM

Abstract
Description
Claims
Application Information

- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com