Anti-sloughing filtrate reducer white asphalt for drilling fluid
A fluid loss control agent and drilling fluid technology, applied in the field of petroleum drilling fluids, can solve the problems of poor anti-slump lubrication performance, great influence on the rheological properties of the mud system, and easy thickening.
- Summary
- Abstract
- Description
- Claims
- Application Information
 AI Technical Summary 
Problems solved by technology
Method used
Examples
Embodiment 1
[0038] White bitumen, an anti-slump and fluid loss reducer for drilling fluid, is processed and prepared from raw materials with the following weight components:
[0039] 6 parts of mixing particles, 0.8 parts of resin filler and 4 parts of copolymerization additives;
[0040] The preparation method of the anti-slump and fluid loss reducer white asphalt for drilling fluid is as follows:
[0041] In the first step, after uniformly mixing high-carbon fatty acids, high-carbon fatty alcohols and polyols in a weight ratio of 23:21:8, stirring and reacting at a temperature of 85°C for 5 hours, adding modified light calcium carbonate to it, mixing After stirring evenly, keep warm and continue to react for 1-3 hours to obtain a liquid phase mixture for use;
[0042]The high-carbon fatty acid is prepared by uniformly mixing lauric acid, palmitic acid and stearic acid in a weight ratio of 0.6:0.9:2.1;
[0043] The high-carbon fatty alcohol is made by uniformly mixing lauryl alcohol, p...
Embodiment 2
[0063] White bitumen, an anti-slump and fluid loss reducer for drilling fluid, is processed and prepared from raw materials with the following weight components:
[0064] 6 parts of mixing particles, 1.3 parts of resin filler and 4 parts of copolymerization additive;
[0065] The preparation method of the anti-slump and fluid loss reducer white asphalt for drilling fluid is as follows:
[0066] In the first step, after uniformly mixing high-carbon fatty acids, high-carbon fatty alcohols and polyols in a weight ratio of 23:21:8, stirring and reacting at a temperature of 85°C for 5 hours, adding modified light calcium carbonate to it, mixing After stirring evenly, keep warm and continue to react for 1-3 hours to obtain a liquid phase mixture for use;
[0067] The high-carbon fatty acid is prepared by uniformly mixing lauric acid, palmitic acid and stearic acid in a weight ratio of 0.6:0.9:2.1;
[0068] The high-carbon fatty alcohol is made by uniformly mixing lauryl alcohol, p...
PUM
 Login to View More
 Login to View More Abstract
Description
Claims
Application Information
 Login to View More
 Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com